2380 | 2378 | 2382 | 2385 | 2383 | 2386 | 2381 | 2379 | 2388 | 2466 | 2461 | 2470 | 2469 | 2452 | 2463 | 2455 | 2454 | 2460 | 2458 | 2465 | 2467 | 2457 | 2436 | 2437 | 2444 | 2447 | 2441 | 2448 | 2428 | 2340 | 2342 | 2358 | 2393 | 2397 | 2398 | 2400 | 2402 | 2403 | 2406 | 2416 | 2414 | 2409 | 2415 | 2411 | 2433 | 2422 | 2429 | 2431 | 2432 | 2361 | 2476 | 2477 | 2478 | 2489 | 2487 | 2490 | 2493 | 2488 | 2491 | 2479 | 2480 | 2474 | 2475 | 2350 | 2362 | 2367 | 2369 | 2355 | 2366 | 2345 | 2346 | 2352 | 2353 | 2394 | 2392 | 2391 | 2360 | 2343 | 2430 | 2453 | 2456 | 2462 | 2442 | 2446 | 2472 | 2471 | 2389 | 2505 | 2499 | 2510 | 2507 | 2511 | 2514 | 2504 | 2417 | 2376 | 2374 | 2375 | 2275 | 2549 | 2541 | 2537 | 2551 | 2538 | 2540 | 2539 | 2542 | 2543 | 2547 | 2546 | 2550 | 2545 | 2544 | 2533 | 2518 | 2531 | 2525 | 2527 | 2522 | 2529 | 2535 | 2556 | 2559 | 2562 | 2563 | 2565 | 2567 | 2568 | 2570 | 2571 | 2572 | 2574 | 2573 | 2558 | 2586 | 2585 | 2584 | 2583 | 2582 | 2588 | 2577 | 2576 | 2575 | 2591 | 2592 | 2587 | 2548 | 2368 | 2371 | 2532 | 2372 | 2520 | 2523 | 2405 | 2401 | 2459 | 2344 | 2341 | 2553 | 2561 | 2581 | 2580 | 2579 | 2578 | 2384 | 2348 | 2351 | 2390 | 2359 | 2339 | 2347 | 2404 | 2425 | 2424 | 2426 | 2427 | 2420 | 2419 | 2418 | 2281 | 2423 | 2421 | 2438 | 2443 | 2445 | 2440 | 2451 | 2481 | 2482 | 2484 | 2483 | 2485 | 2495 | 2508 | 2509 | 2552 | 2370 | 2594 | 2373 | 2516 | 2554 | 2502 | 2494 | 2410 | 2407 | 2408 | 2569 | 2557 | 2519 | 2357 | 2503 | 2530 | 2349 | 2289 | 2536 | 2560 | 2555 | 2521 | 2589 | 2515 | 2601 | 2603 | 2604 | 2605 | 2606 | 2607 | 2608 | 2609 | 2610 | 2611 | 2612 | 2613 | 2513 | 2614 | 2615 | 2616 | 2617 | 2618 | 2619 | 2620 | 2621 | 2622 | 2623 | 2624 | 2625 | 2626 | 2627 | 2628 | 2629 | 2630 | 2631 | 2632 | 2633 | 2634 | 2602 | 2635 | 2636 | 2637 | 2639 | 2640 | 2642 | 2643 | 2449 | 2399 | 2387 | 2354 | 2377

These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.

Black silky matte MNS mug

Serial Number: AJ24314
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Black
Clay Body - L4208C MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 107 mm (4.2 in)
Weight - 334 grams (11.8 oz)

Price: $40.00 - Buy it