Monthly Tech-Tip | No tracking! No ads! |
These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24145
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2826B
Glaze Outside - G2934Y Orange
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 124 mm (4.9 in)
Weight - 392 grams (13.8 oz)
Reluctantly Sold
Buy me a coffee and we can talk