These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24322
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571B
Engobe - L3954N
Clay Body - H450
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 113 mm (4.4 in)
Weight - 424 grams (14.9 oz)