These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ50013
Run/Test Number: L4449J
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G3933E
Clay Body - Coffee Clay
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 98 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 123 mm (4.8 in)
Weight - 418 grams (14.7 oz)
Not for sale