These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24358
Run/Test Number: L4382A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Description: This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571B bamboo matte
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 106 mm (4.2 in)
Weight - 360 grams (12.7 oz)