2380 | 2378 | 2382 | 2387 | 2377 | 2385 | 2383 | 2386 | 2381 | 2379 | 2388 | 2466 | 2461 | 2470 | 2469 | 2452 | 2463 | 2455 | 2454 | 2460 | 2458 | 2465 | 2467 | 2457 | 2436 | 2437 | 2444 | 2447 | 2441 | 2448 | 2428 | 2340 | 2342 | 2354 | 2358 | 2393 | 2397 | 2398 | 2399 | 2400 | 2402 | 2403 | 2406 | 2416 | 2414 | 2409 | 2415 | 2411 | 2433 | 2422 | 2429 | 2431 | 2432 | 2361 | 2476 | 2477 | 2478 | 2489 | 2487 | 2490 | 2493 | 2488 | 2491 | 2479 | 2480 | 2474 | 2475 | 2350 | 2362 | 2367 | 2369 | 2355 | 2366 | 2345 | 2346 | 2352 | 2353 | 2394 | 2392 | 2391 | 2360 | 2343 | 2430 | 2453 | 2456 | 2462 | 2442 | 2446 | 2472 | 2471 | 2389 | 2505 | 2499 | 2510 | 2507 | 2511 | 2514 | 2504 | 2417 | 2376 | 2374 | 2375 | 2275 | 2549 | 2541 | 2537 | 2551 | 2538 | 2540 | 2539 | 2542 | 2543 | 2547 | 2546 | 2550 | 2545 | 2544 | 2533 | 2518 | 2531 | 2525 | 2527 | 2522 | 2529 | 2535 | 2556 | 2559 | 2562 | 2563 | 2565 | 2567 | 2568 | 2570 | 2571 | 2572 | 2574 | 2573 | 2558 | 2586 | 2585 | 2584 | 2583 | 2582 | 2588 | 2577 | 2576 | 2575 | 2591 | 2592 | 2587 | 2548 | 2368 | 2371 | 2532 | 2372 | 2520 | 2523 | 2405 | 2401 | 2459 | 2344 | 2341 | 2553 | 2561 | 2581 | 2580 | 2579 | 2578 | 2384 | 2348 | 2351 | 2390 | 2359 | 2339 | 2347 | 2404 | 2425 | 2424 | 2426 | 2427 | 2420 | 2419 | 2418 | 2281 | 2423 | 2421 | 2438 | 2443 | 2445 | 2440 | 2451 | 2481 | 2482 | 2484 | 2483 | 2485 | 2495 | 2508 | 2509 | 2552 | 2370 | 2594 | 2373 | 2516 | 2554 | 2502 | 2494 | 2410 | 2407 | 2408 | 2569 | 2557 | 2519 | 2357 | 2503 | 2530 | 2349 | 2289 | 2536 | 2560 | 2555 | 2521 | 2589 | 2515 | 2601 | 2603 | 2604 | 2605 | 2606 | 2607 | 2608 | 2609 | 2610 | 2611 | 2612 | 2613 | 2513 | 2614 | 2615 | 2616 | 2617 | 2618 | 2619 | 2620 | 2621 | 2622 | 2623 | 2624 | 2625 | 2626 | 2627 | 2628 | 2629 | 2630 | 2631 | 2632 | 2633 | 2634 | 2602 | 2635 | 2636 | 2637 | 2639 | 2640 | 2642 | 2643 | 2449

These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.

Floating-blue stoneware mug

Serial Number: AJ24361
Run/Test Number: L4471D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GR6-M
Glaze Outside - PLC6DS
Clay Body - M390 test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 109 mm (4.3 in)
Weight - 348 grams (12.3 oz)