These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24330
Run/Test Number: P6882
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2880A
Glaze Outside - G2880A Tenmoku
Clay Body - P600
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 103 mm (4.1 in)
Weight - 347 grams (12.2 oz)