These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24077
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C
Clay Body - M350
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 116 mm (4.6 in)
Weight - 431 grams (15.2 oz)
Price: $35.00 - Buy it