Monthly Tech-Tip | No tracking! No ads! |
These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ240160
Run/Test Number: L4249A
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-A
Glaze Outside - GA6-C
Clay Body - L4249A MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 124 mm (4.9 in)
Weight - 425 grams (15.0 oz)
Price: $55.00 - Buy it