These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24327
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A bamboo matte
Engobe - L3954N
Clay Body - H450
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 112 mm (4.4 in)
Depth at rim (including handle) - 138 mm (5.4 in)
Height - 122 mm (4.8 in)
Weight - 418 grams (14.7 oz)