Monthly Tech-Tip | No tracking! No ads! |
These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24363
Run/Test Number: L4471G
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GR6-M
Clay Body - M390 test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 123 mm (4.8 in)
Weight - 369 grams (13.0 oz)
Price: $35.00 - Buy it
Buy me a coffee and we can talk