These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24422
Run/Test Number: L4453E
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - GR10-CW
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 108 mm (4.3 in)
Weight - 350 grams (12.3 oz)
Price: $45.00 - Buy it