These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24306
Run/Test Number: P6904
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GA6-B
Engobe - L3954B
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 98 mm (3.9 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 110 mm (4.3 in)
Weight - 396 grams (14.0 oz)