2380 | 2378 | 2382 | 2385 | 2383 | 2386 | 2381 | 2379 | 2388 | 2466 | 2461 | 2470 | 2469 | 2452 | 2463 | 2455 | 2454 | 2460 | 2458 | 2465 | 2467 | 2457 | 2436 | 2437 | 2444 | 2447 | 2441 | 2448 | 2428 | 2340 | 2342 | 2358 | 2393 | 2397 | 2398 | 2400 | 2402 | 2403 | 2406 | 2416 | 2414 | 2409 | 2415 | 2411 | 2433 | 2422 | 2429 | 2431 | 2432 | 2361 | 2476 | 2477 | 2478 | 2489 | 2487 | 2490 | 2493 | 2488 | 2491 | 2479 | 2480 | 2474 | 2475 | 2350 | 2362 | 2367 | 2369 | 2355 | 2366 | 2345 | 2346 | 2352 | 2353 | 2394 | 2392 | 2391 | 2360 | 2343 | 2430 | 2453 | 2456 | 2462 | 2442 | 2446 | 2472 | 2471 | 2389 | 2505 | 2499 | 2510 | 2507 | 2511 | 2514 | 2504 | 2417 | 2376 | 2374 | 2375 | 2275 | 2549 | 2541 | 2537 | 2551 | 2538 | 2540 | 2539 | 2542 | 2543 | 2547 | 2546 | 2550 | 2545 | 2544 | 2533 | 2518 | 2531 | 2525 | 2527 | 2522 | 2529 | 2535 | 2556 | 2559 | 2562 | 2563 | 2565 | 2567 | 2568 | 2570 | 2571 | 2572 | 2574 | 2573 | 2558 | 2586 | 2585 | 2584 | 2583 | 2582 | 2588 | 2577 | 2576 | 2575 | 2591 | 2592 | 2587 | 2548 | 2368 | 2371 | 2532 | 2372 | 2520 | 2523 | 2405 | 2401 | 2459 | 2344 | 2341 | 2553 | 2561 | 2581 | 2580 | 2579 | 2578 | 2384 | 2348 | 2351 | 2390 | 2359 | 2339 | 2347 | 2404 | 2425 | 2424 | 2426 | 2427 | 2420 | 2419 | 2418 | 2281 | 2423 | 2421 | 2438 | 2443 | 2445 | 2440 | 2451 | 2481 | 2482 | 2484 | 2483 | 2485 | 2495 | 2508 | 2509 | 2552 | 2370 | 2594 | 2373 | 2516 | 2554 | 2502 | 2494 | 2410 | 2407 | 2408 | 2569 | 2557 | 2519 | 2357 | 2503 | 2530 | 2349 | 2289 | 2536 | 2560 | 2555 | 2521 | 2589 | 2515 | 2601 | 2603 | 2604 | 2605 | 2606 | 2607 | 2608 | 2609 | 2610 | 2611 | 2612 | 2613 | 2513 | 2614 | 2615 | 2616 | 2617 | 2618 | 2619 | 2620 | 2621 | 2622 | 2623 | 2624 | 2625 | 2626 | 2627 | 2628 | 2629 | 2630 | 2631 | 2632 | 2633 | 2634 | 2602 | 2635 | 2636 | 2637 | 2639 | 2640 | 2642 | 2643 | 2449 | 2399 | 2387 | 2354 | 2377

These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.

Variegated blue porcelain mug

Serial Number: AJ24333
Run/Test Number: P6929
Technique: Thrown, dip glazed.

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571F
Glaze Outside - G2571F blue matte
Clay Body - P580
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 118 mm (4.6 in)
Weight - 358 grams (12.6 oz)

Price: $35.00 - Buy it