Monthly Tech-Tip | No tracking! No ads! |
These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ50022
Run/Test Number: L4686C
Description: Fired at cone 6 oxidation on buff stoneware. By Tony Hansen.
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571D Red
Clay Body - H570
Foot Style - Flat unglazed
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 102 mm (4.0 in)
Weight - 313 grams (11.0 oz)
Not for sale
Buy me a coffee and we can talk