Zirconium (Zr) constitutes about 0.2% of the earth039;s crust, common minerals bind zircon, zirconium dioxide and zirconates.
Potential occupational exposures to zirconium may be encountered during:
Zirconium compounds are generally considered to be of low toxicity.
Granulomata have been produced by repeated topical applications of zirconium salts to human skin.
Zirconium compounds are commonly used in antiperspirants and thus sometimes cause granulomata of the axillary skin. Aluminium zirconium compounds, which are mainly used today, are considered to be safer in this regard.
Studies among workers exposed to zirconium compounds fumes have failed to demonstrate adverse pulmonary effects.
However, a recent report shows that severe pulmonary fibrosis containing high concentrations of several zirconium compounds occurred in a worker polishing and blocking lenses in an optical company.
In my personal experience I have encountered a corneal burn with a subsequent scar in a titanium dioxide plant caused by the ocular projection of a small drop of liquid zirconium sulfate at the place where it was introduced into the process.
VEMP (Valeur d039;Exposition Moyenne Pondérée) = 5mg/m³
By Edouard Bastarache
| Hazards |
Zirconium Encapsulated Stains Toxicity
|
| Materials |
Magnesium Zirconium Silicate
|
| Materials |
Zircon
Zircon (zirconium silicate) is a hard, dense, refractory ceramic material used to opacify pottery glazes and in refractory products such as kiln washes, crucibl |
| Materials |
Zircopax
Zirconium silicate, its principle use in ceramics is as an opacifier in glazes. It is an expensive material, but less so than tin oxide. |
| Materials |
Superpax
|
| Typecodes |
Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk