BORY1 - Bory 1 Crystalline Glaze
CELECG - Celestite Crystalline Glaze
FAAO - Fa's All-Opaque Crystalline Glaze
FAC5 - Crystal Number Five Glaze
FO - Octal Crystalline Glaze
G1214M - 20x5 Cone 6 Base Glossy Glaze
G1214W - Cone 6 Transparent Base
G1214Z1 - Cone 6 Silky CaO matte base glaze
G1215U - Low Expansion Glossy Clear Cone 6
G1216L - Transparent for Cone 6 Porcelains
G1216M - Cone 6 Ultraclear Glaze for Porcelains
G1916Q - Low Fire Highly-Expansion-Adjustable Transparent
G1947U - Cone 10 Glossy transparent glaze
G2000 - LA Matte Cone 6 Matte White
G2240 - Cone 10R Classic Spodumene Matte
G2571A - Cone 10 Silky Dolomite Matte glaze
G2826R - Floating Blue Cone 5-6 Original Glaze Recipe
G2826X - Randy's Red Cone 5
g2851H - Ravenscrag Cone 6 High Calcium Matte Blue
G2853B - Cone 04 Clear Ravenscrag School Glaze
G2896 - Ravenscrag Plum Red Cone 6
G2902B - Cone 6 Crystal Glaze
G2902D - Cone 6 Crystalline Development Project
G2916F - Cone 6 Stoneware/Whiteware transparent glaze
G2926B - Cone 6 Whiteware/Porcelain transparent glaze
G2926J - Low Expansion G2926B
G2928C - Ravenscrag Silky Matte for Cone 6
G2931H - Ulexite High Expansion Zero3 Clear Glaze
G2931K - Low Fire Fritted Zero3 Transparent Glaze
G2931L - Low Expansion Low-Fire Clear
G2934 - Matte Glaze Base for Cone 6
G2934Y - Cone 6 Magnesia Matte Low LOI Version
G3806C - Cone 6 Clear Fluid-Melt transparent glaze
G3838A - Low Expansion Transparent for P300 Porcelain
G3879 - Cone 04 Transparent Low-Expansion transparent glaze
GA10-A - Alberta Slip Base Cone 10R
GA10-B - Alberta Slip Tenmoku Cone 10R
GA10-D - Alberta Slip Black Cone 10R
GA10x-A - Alberta Slip Base for cone 10 oxidation
GA6-A - Alberta Slip Cone 6 transparent honey glaze
GA6-B - Alberta Slip Cone 6 transparent honey glaze
GA6-C - Alberta Slip Floating Blue Cone 6
GA6-D - Alberta Slip Glossy Brown Cone 6
GA6-F - Alberta Slip Cone 6 Oatmeal
GA6-G - Alberta Slip Lithium Brown Cone 6
GA6-G1 - Alberta Slip Lithium Brown Cone 6 Low Expansion
GA6-H - Alberta Slip Cone 6 Black
GBCG - Generic Base Crystalline Glaze
GC106 - GC106 Base Crystalline Glaze
GR10-A - Pure Ravenscrag Slip
GR10-B - Ravenscrag Cone 10R Gloss Base
GR10-C - Ravenscrag Cone 10R Silky Talc Matte
GR10-E - Alberta Slip:Ravenscrag Cone 10R Celadon
GR10-G - Ravenscrag Cone 10 Oxidation Variegated White
GR10-J - Ravenscrag Cone 10R Dolomite Matte
GR10-J1 - Ravenscrag Cone 10R Bamboo Matte
GR10-K1 - Ravenscrag Cone 10R Tenmoku
GR10-L - Ravenscrag Iron Crystal
GR6-A - Ravenscrag Cone 6 Clear Glossy Base
GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue
GR6-C - Ravenscrag Cone 6 White Glossy
GR6-D - Ravenscrag Cone 6 Glossy Black
GR6-E - Ravenscrag Cone 6 Raspberry Glossy
GR6-H - Ravenscrag Cone 6 Oatmeal Matte
GR6-L - Ravenscrag Cone 6 Transparent Burgundy
GR6-M - Ravenscrag Cone 6 Floating Blue
GR6-N - Ravenscrag Alberta Brilliant Cone 6 Celadon
GRNTCG - GRANITE Crystalline Glaze
L2000 - 25 Porcelain
L3341B - Alberta Slip Iron Crystal Cone 10R
L3685U - Cone 03 White Engobe Recipe
L3724F - Cone 03 Terra Cotta Stoneware
L3924C - Zero3 Porcelain Experimental
L3954B - Cone 6 Engobe for Stonewares
L3954N - Cone 10R Base White Engobe Recipe for stonewares
MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
MGBase6 - Zinc Semimatte Glossy Base Cone 6
MGBase7 - Raspberry Cone 6 (Mastering Glazes)
MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
TNF2CG - Tin Foil II Crystalline Glaze
VESUCG - Vesuvius Crystalline Glaze

Insight-Live Shares (also referencing this recipe)

These add technical detail, development info, variations and improvements.

L3954B - Cone 6 White Engobe Recipe

Modified: 2026-06-15 03:33:31

Drying and firing shrinkage fitted to Plainsman M390, M340

Material Amount Percent
Nepheline Syenite18.0020.7
Silica15.0017.2
OM #4 Ball Clay54.0062.1
Added
Zircopax10.0011.49
Bentonite3.003.45
100.00 100

Notes

This is white because of the 10% Zircopax. Increase that 20% for maximum white. The black version of this is L3954F.

This recipe has been tuned to have about the same fired shrinkage as a stoneware at cone 6 (I measure this at 6.7% dry-to-fired shrinkage using the SHAB test). I also confirmed fired-shrinkage-match using the EBCT test). If the body you use has between 6.5 and 7.0 fired shrinkage, this should work. Do not ignore this detail. If you apply this as an engobe (e.g. by dipping leather-hard functional pieces), and it is not firing-shrinkage-compatible with the body, it could eventually flake off during use.

The color is whiter than previous trials (because of the zircopax), but some might prefer a little blue stain to brighten the color. I used 0.2% Mason 6336 with success; other stains I tried agglomerated and caused specking. For a super-white see the L3954R recipe.

As with other engobes, I recommend mixing in a kitchen blender; it is an ideal way to get the lumps out and thoroughly wet all particle surfaces.

A thixotropic dipping slurry is needed and I have found it is possible to create a deflocculated one using 1000 powder, 780g water, ~3g Darvan. This produces a specific gravity of ~1.55. If it is too viscous add more Darvan, too fluid add a tiny amount of Epsom salts to bring it back to a creamy texture.

A brushing version can also be made, see the notes for the L3954F black engobe.

Related Information

A white engobe on dark and buff burning cone 6 stonewares


This picture has its own page with more detail, click here to see it.

Left is Plainsman M340. Right is M390. Each mug has been white-engobed inside (by pouring), using L3954B, and halfway down the outside (by dipping). The insides have been glazed using G2926B clear. The inside surface has more depth and a richer appearance than could be achieved using a white glaze (especially over the dark burning body). The outside of the left one is Alberta Slip base GA6-B. The outside glaze on the right is the clear plus 4% iron oxide. This technique of using the engobe enables porcelain-like functional surfaces on the insides and the visual contrasts and character on the outsides of the stoneware mugs.

Thickly applied slips must fit the body and each other


Pottery slips are flaking off during drying

This picture has its own page with more detail, click here to see it.

Fit? It has to stick well. And stay stuck during drying (and shrinking). And the bond has to survive shrinkage that happens during firing. This potter is doing thick applications of each slip (actually that makes them engobes). She uses stains, that's wise, metal oxides bring baggage when used to color slips (e.g. their decomposition can affect the bond, they can gel the slurry, flux the fired product thereby increasing the firing shrinkage of the slip). Stains are better because they affect slurry and fired properties less. But there are still enough issues that each colored slip deserves testing. This potter first slaked B-mix as a slip (it is highly plastic), using it at a runny yogurt consistency. But it bubbled when fired hotter than a cool cone 6. A switch to porcelain slip (which is non-plastic) is shown here. It flaked off as it dried (even in a damp box for 24 hours), also after bisquing to cone 08, and sometimes even after firing to cone 6. This signalled a drying mismatch between body and slip, the bond that managed to survive drying was weakened enough to fail on firing.

The solution was an engobe recipe that is super plastic and sticky. The popular Fish Sauce recipe is an example, it contains 10% bentonite and is unbelievably sticky. L3954B was formulated with this in mind. It adheres well to leather-hard clay and doesn't flake off (misfit is instead evident by surface cracking if its shrinks more than the body). And it is not highly vitreous, keeping its fired shrinkage low enough to match stoneware bodies. Mixing your own recipe also enables compensating the amount of feldspar if the stain affects the slip's degree of vitrification, and therefore fired shrinkage (e.g. blues, oranges, yellows).

Can an engobe block manganese speckle at cone 6?


Engobe blocking manganese speckle

This picture has its own page with more detail, click here to see it.

Yes. If it is a true engobe. This is L3954B fired at cone 6 on Plainsman M340S, it is fire-shrinkage-fitted to this clay body and opacified with Zircopax. The cover glaze is G2926B transparent. The opacity that this engobe is able to achieve here is because it is vitrifying to the same degree as the body, no melting is occurring and that is why it is completely opaque (even though it is applied as a very thin layer at the leather hard stage). This same performance could be expected in reduction firings to block the iron speckle (using the L3954N and variations recipes).

Cone 6 engobe becomes super white with 20% zircon added


Engobe with 20% zircon.

This picture has its own page with more detail, click here to see it.

Engobes were applied to the insides, and up over the rim, of these M340 pieces at the leather hard stage. They were then bisque fired, clear glazed and fired to cone 6. On the left is L3954B, no zircon was added. The one on the right is L3954S2, in has 20% Zircopax. These are part of a fitting effort to match the firing shrinkage of the body, M340, to a base engobe (and colored versions of it).

Absolutely Jet-Black Cone 6 Engobe on M340

This could also be super white


A buff stoneware mug with black engobe

This picture has its own page with more detail, click here to see it.

This is the L3954B engobe. 15% Mason 6600 black body stain has been added (instead of the normal 10% Zircopax used for white). Of course, a cover glaze is needed for a functional surface. A lot of development work went into producing a recipe that fits this body, M340. It works even when thickly applied because it has the same fired maturity as the body. Lots of information is available on using L3954B (including mixing and adjustment instructions). Engobes are tricky to use. Follow the links below to learn more. L3954B is designed to work on regular Plainsman M340 (this piece), M390 and Coffee Clay. Most importantly, adjusting its maturity, and thus reducing firing shrinkage, is documented. These bodies dry better than porcelains and are much less expensive, so coating them with an engobe to get a surface like this makes a lot of sense. Ed Phillipson discovered this 80 years ago, enabling selling pieces made from these clays as white hotelware.

A black engobe transforms the floating blue glaze over it


Floating blue over black engobe

This picture has its own page with more detail, click here to see it.

This is M340 stoneware fired to cone 6 using the C6DHSC schedule. The L3954B engobe fires deep black (it has 10% Mason 6600 black stain). The engobe was applied by pouring and dipping at leather hard stage (inside and partway down the outside). After bisque firing, the piece was glazed inside using the base GA6-B Alberta Slip amber base. The outside glaze is Alberta Slip Rutile Blue GA6-C (you are seeing it on the bare buff body near the bottoms and over the black clay surface on the uppers).

A cone 6 black-burning stoneware with a porcelain surface. How?


A black stoneware mug

This picture has its own page with more detail, click here to see it.

Black-burning bodies are popular with many potters. This one is stained by adding 10% raw umber to a buff-burning stoneware. Umbers are powerful natural clay colorants, they have high iron and also contain some manganese oxide. Could a white engobe produce a porcelain-like surface on such a clay body? Yes. L3954B engobe was applied during leather-hard stage to this Plainsman Coffee Clay mug (on the inside and partway down the outside). After bisque, transparent G2926B glaze was applied inside and GA6-B outside. Notice the GA6-B over the engobe fires amber but over the black it produces a deep glossy brown. The engobe was mixed into a thixotropic slurry, as explained on the page at PlainsmanClays.com (see link below), and applied in a relatively thin layer. This porcelain-like result is a testament to the covering power of a true engobe. It is no wonder they are so popular in the ceramic tile industry - a red-burning body can be turned white as a porcelain, which enables all the marvellous glazing and decorating they can do.

Dark Umber-Stained Engobes on M340 at cone 6


This picture has its own page with more detail, click here to see it.

This is the standard Plainsman L3954D white engobe recipe with the 10% Zircopax switched for Burnt Umber. The result is a dark, rich, ultra-gloss brown (almost black). The engobe is applied inside and half-way down the outside. The mug on the left is glazed inside and out with the base GA6A Alberta Slip cone 6 recipe (but uses Ferro Frit 3195 instead of 3134). The one on the right has the same glaze on the outside but the G2926B clear transparent on the inside (it is micro-bubbling). This engobe works even better with a black stain.

Stage 1 of engobing a cone 6 red stoneware mug


This picture has its own page with more detail, click here to see it.

On the right is what it will look like when fired with a clear glaze on the inside and amber-clear on the outside. On the left it has dried and is ready for a little fix-up before bisque firing.

Worst case scenario for handle joins and successful drying


Leather hard mugs with waxed handles

This picture has its own page with more detail, click here to see it.

These M390 mugs had progressed to stiff leather hard (after handles were applied, using just slip, and bases trimmed). A white engobe was then applied to the inside. It significantly softened the bodies of the mugs (to re-dry them to the point of being able to turn them over takes 4-6 more hours). This process sets up a big moisture differential between the mug and handle. "Even drying" is the key to success, so slowing down the handles is obviously needed. How? I apply wax emulsion (actually, I like Reed Wax), leaving just the inside handle-curves bare. That slows down drying enough to keep them even with the body of the mug. This method works so well that these do not even need covering during drying (even in our desert climate). Even drying is the goal - fast and even drying is much better than slow and uneven.

GA6A Alberta Slip base using Frit 3249 and 3195 on buff body


This picture has its own page with more detail, click here to see it.

The body is buff burning Plainsman M340 (cone 6). The amber colored glaze is 80% Alberta Slip (raw:calcine mix) with 20% of each frit. The white engobe on the inside of mug 1 is L3954A (also glazed inside using transparent G2926B). These frits are producing an amber gloss glaze of high quality. On the outside of mug 1 we see the 3195 version on the white slip until midway down, then on the bare buff clay (the other has the 3249 version). These mugs are fired using a drop-and-soak firing schedule. A couple of caveats: Frit 3249 has a very low thermal expansion, use it on bodies that craze other glazes (like Plainsman P300), it could shiver on stonewares like this. Both of these frits prevent the formation of bloating blues (with additions of rutile or titanium).

A cone 6 clear glaze plus iron vs. Alberta Slip amber base


This picture has its own page with more detail, click here to see it.

These two mugs are made from a dark red burning stoneware and fired in a cool-and-soak firing schedule. A white engobe (L3954A) has been applied on the inside and half way down the outside. Both are glazed inside with G2926B whiteware transparent glaze. The outside glaze on the left is the same transparent with 4% added iron oxide. It has been sieved to 80 mesh. Notice the iron agglomerates and still produces specking (an effect that may be desired, but difficult to keep consistent). Interestingly, that iron is producing a clear amber-colored glass about equal in color to the Alberta Slip GA6A base glaze (80% Alberta Slip, 20% Frit 3195) on the mug on the right. Neither has the micro bubbles that mar a typical clear glaze on bodies like this.

Four drops of Davan deflocculant fixed the problem!


This picture has its own page with more detail, click here to see it.

This is a white engobe (L3954B) drying on two dark burning cone 6 stoneware leather-hard mugs (Plainsman M390). Those lumps are on the left cannot be screened out, they are agglomerates. That slip has excessive flocculant (powdered Epsom salts are added to gel it so that it stays put on the piece after dipping). About 4 drops of Darvan were added to one gallon of the slurry, this immediately made it smooth and a perfect consistency for application. It remains stable on ware (without runs). Engobes require tight control to have the right viscosity and thixotropy (which can be achieved over a range of specific gravities (about 1.45-1.6). When they are right they are a joy to use, when they are not ware is ruined.

Here is what dipping engobes can do:

Go on even. In one coat. Stay put.


This picture has its own page with more detail, click here to see it.

When you learn to make and use engobes correctly, they make magic possible. Here I am turning a dark rustic body into a smooth white one (rear mugs) and a white body into a dark one (front). The engobes have been applied at the leather-hard stage. That is the perfect time, the engobe and body are clay bodies, designed to fit each other; they dry together and fire together creating an inseparable bond.

Handles have been applied, and they have dried to stiff leather hard. Engobe was poured in, poured out, then the mugs were pressed, lip down, into it and extracted. No dwell time was needed. This dipping engobe is DIY thixotropic (not available commercially anywhere). That means I tuned it just before use, to just the right degree of gel (enough for it to drain to the right thickness, then gel just as the last few drops fall from the rim). Honestly, these are a beauty to behold at this stage, the silky, drip-free surface is just so perfect.

Links

URLs https://insight-live.com/insight/share.php?z=uiqNgtxwws
White Cone 6 Engobe, New Alberta Slip glazes, Firing Schedule

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

XML to Paste Into Insight-live

<?xml version="1.0"?>
<recipes version="1.0" encoding="UTF-8">
<recipe name="Cone 6 White Engobe Recipe" keywords="Drying and firing shrinkage fitted to Plainsman M390, M340" id="134" date="2026-06-15" codenum="L3954B">
<recipelines>
<recipeline material="Nepheline Syenite" amount="18.000"/>
<recipeline material="Silica" amount="15.000"/>
<recipeline material="OM #4 Ball Clay" amount="54.000"/>
<recipeline material="Zircopax" amount="10.000" added="1"/>
<recipeline material="Bentonite" amount="3.000" added="1"/>
<url url="https://backup.digitalfire.com/recipe/134" descrip="https://backup.digitalfire.com/recipe/134"/>
</recipelines>
<urls/>
</recipe>
</recipes>
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy