BORY1 - Bory 1 Crystalline Glaze
CELECG - Celestite Crystalline Glaze
FAAO - Fa's All-Opaque Crystalline Glaze
FAC5 - Crystal Number Five Glaze
FO - Octal Crystalline Glaze
G1214M - 20x5 Cone 6 Base Glossy Glaze
G1214W - Cone 6 Transparent Base
G1214Z1 - Cone 6 Silky CaO matte base glaze
G1215U - Low Expansion Glossy Clear Cone 6
G1216L - Transparent for Cone 6 Porcelains
G1216M - Cone 6 Ultraclear Glaze for Porcelains
G1916Q - Low Fire Highly-Expansion-Adjustable Transparent
G1947U - Cone 10 Glossy transparent glaze
G2000 - LA Matte Cone 6 Matte White
G2240 - Cone 10R Classic Spodumene Matte
G2571A - Cone 10 Silky Dolomite Matte glaze
G2826R - Floating Blue Cone 5-6 Original Glaze Recipe
G2826X - Randy's Red Cone 5
g2851H - Ravenscrag Cone 6 High Calcium Matte Blue
G2853B - Cone 04 Clear Ravenscrag School Glaze
G2896 - Ravenscrag Plum Red Cone 6
G2902B - Cone 6 Crystal Glaze
G2902D - Cone 6 Crystalline Development Project
G2916F - Cone 6 Stoneware/Whiteware transparent glaze
G2926B - Cone 6 Whiteware/Porcelain transparent glaze
G2926J - Low Expansion G2926B
G2928C - Ravenscrag Silky Matte for Cone 6
G2931H - Ulexite High Expansion Zero3 Clear Glaze
G2931K - Low Fire Fritted Zero3 Transparent Glaze
G2931L - Low Expansion Low-Fire Clear
G2934 - Matte Glaze Base for Cone 6
G2934Y - Cone 6 Magnesia Matte Low LOI Version
G3806C - Cone 6 Clear Fluid-Melt transparent glaze
G3838A - Low Expansion Transparent for P300 Porcelain
G3879 - Cone 04 Transparent Low-Expansion transparent glaze
GA10-A - Alberta Slip Base Cone 10R
GA10-B - Alberta Slip Tenmoku Cone 10R
GA10-D - Alberta Slip Black Cone 10R
GA10x-A - Alberta Slip Base for cone 10 oxidation
GA6-A - Alberta Slip Cone 6 transparent honey glaze
GA6-B - Alberta Slip Cone 6 transparent honey glaze
GA6-C - Alberta Slip Floating Blue Cone 6
GA6-D - Alberta Slip Glossy Brown Cone 6
GA6-F - Alberta Slip Cone 6 Oatmeal
GA6-G - Alberta Slip Lithium Brown Cone 6
GA6-G1 - Alberta Slip Lithium Brown Cone 6 Low Expansion
GA6-H - Alberta Slip Cone 6 Black
GBCG - Generic Base Crystalline Glaze
GC106 - GC106 Base Crystalline Glaze
GR10-A - Pure Ravenscrag Slip
GR10-B - Ravenscrag Cone 10R Gloss Base
GR10-C - Ravenscrag Cone 10R Silky Talc Matte
GR10-E - Alberta Slip:Ravenscrag Cone 10R Celadon
GR10-G - Ravenscrag Cone 10 Oxidation Variegated White
GR10-J - Ravenscrag Cone 10R Dolomite Matte
GR10-J1 - Ravenscrag Cone 10R Bamboo Matte
GR10-K1 - Ravenscrag Cone 10R Tenmoku
GR10-L - Ravenscrag Iron Crystal
GR6-A - Ravenscrag Cone 6 Clear Glossy Base
GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue
GR6-C - Ravenscrag Cone 6 White Glossy
GR6-D - Ravenscrag Cone 6 Glossy Black
GR6-E - Ravenscrag Cone 6 Raspberry Glossy
GR6-H - Ravenscrag Cone 6 Oatmeal Matte
GR6-L - Ravenscrag Cone 6 Transparent Burgundy
GR6-M - Ravenscrag Cone 6 Floating Blue
GR6-N - Ravenscrag Alberta Brilliant Cone 6 Celadon
GRNTCG - GRANITE Crystalline Glaze
L2000 - 25 Porcelain
L3341B - Alberta Slip Iron Crystal Cone 10R
L3685U - Cone 03 White Engobe Recipe
L3724F - Cone 03 Terra Cotta Stoneware
L3924C - Zero3 Porcelain Experimental
L3954B - Cone 6 Engobe for Stonewares
L3954N - Cone 10R Base White Engobe Recipe for stonewares
MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
MGBase6 - Zinc Semimatte Glossy Base Cone 6
MGBase7 - Raspberry Cone 6 (Mastering Glazes)
MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
TNF2CG - Tin Foil II Crystalline Glaze
VESUCG - Vesuvius Crystalline Glaze

Insight-Live Shares


103-A, 103-B - Lindoe cone 10R blue glaze
111.BG-2 - Lindoe cone 10R blue glaze
77C04E - 50:30:20 Frit 3134 cone 6 base
77E05B - Cone 10R Celadon - Luke Lindoe
77E06B - Lindoe Dark Celadon - Lower COE
77E10A - Lindoe Crackle Glaze - Cone 10R
77E10A1 - 3110 Crackle - Oxidation
77E10A2 - Hybrid Crackle Adjustable
77E14A - Cone 10R Red Mustard - Luke Lindoe
77E15A - Cone 10R Yellow Mustard - Luke Lindoe
78-81-B - Lindoe crystal blue cone 10R glazes
84-40 - Lindoe barium blue cone 10R glaze
84-G-05-S - Cone 10R Matte Crystal Iron - Luke Lindoe
G 304 - Cone 10R Crystal Iron Brown - Luke Lindoe
G1002 - LEACH'S CELADON CONE 10R
G1129 - MEDALTA CLEAR GLAZE CONE 8-10
G1214M - Hansen 20x5 Clear Cone 6 Base Glaze
G1214Z - Cone 6 Calcium Matte Base Glaze
G1214Z1 - Cone 6 Calcium Matte v2
G1214Z2 - Cone 6 Calcium Matte + TiO2
G1847 - Cone 10R Robin's Egg Blue
G1916M - COE Adjustable Low Fire Clear Glaze
G1916Q - Cone 05+ Expansion Adjustable Gloss Base
G1916Q2 - G1916Q glaze + 5% silica
G1916Q3 - G1916Q glaze + 10% silica
G1916QL - Cone 05+ Low Expansion Transparent glaze
G1916QL1 - Cone 05+ Lower Expansion glaze
G1916S - Cone 06-04 MgO Matte
G1916S1 - Cone 06-04 MgO (using talc)
G1916V - Cone 2 Clear (based on G1916Q)
G1916W - G1916Q with Iron Fining Agent
G1947U - Cone 10/10R Transparent Base
G2415E - Classic Albany Lithium Brown Glossy
G2415J - G2415E Alberta Slip Brown (less Li)
G2571A - Original Cone 10R Silky Matte Base Recipe
G2571B - Cone 10R Silky Matte Base (improved)
G2571BB - G2571B Rutile Bamboo
G2571C - Cone 10R Silky Matte Blue
G2571D - Cone 10R Silky Matte Red
G2571D1 - Cone 10 Marbled Red Glaze
G2571E - Cone 10R Silky Matte Black
G2576B - Cone 10R Tenmoku Glossy
G2584 - Cone 10R Blue Celadon
G2826A - 50:30:20 Gerstley Borate Cone 6 base
G2826A1 - 50:30:20 Frit 3134 base (fixed)
G2826A2 - 50:30:20 Gillespie Borate Cone 6 base
G2826A3 - 50:30:20 GB Makeover Pottery Glaze
G2826B - GB:Frit Raku Glaze
G2826F - GB Honey Amber 04
G2826G - GB Lavendar Satin Glaze Cone 6
G2826M - Gerstley Borate Antique Green Cone 5
G2826N - Gerstley Borate Raku Base NS/GB
G2826R - Floating Blue Original Cone 6 Glaze
G2826R1 - Floating Blue Using Gillespie Borate
G2826U - Floating Blue using Frit 3134
G2826V - Gerstley Borate Cream Oatmeal Cone 6 recipe
G2850C - Ravenscrag Cone 6 Black Glossy
G2850M-C - Ravenscrag Cone 6 Light Blue Matte
G2850P - TEAL BLUE CONE 6 KAT
G2851A - RAVENSCRAG SLIP Matte Blue - Cone 6
G2851AB - RAVENS FLOATING BLUE Cone 6
G2851D - KAT'S RC MATTE - Cone 6
G2851H - RAVENSCRAG Brown Gold Matte Cone 6
G2880 - Alberta Slip Tenmoku #1
G2880A - Alberta Slip Tenmoku #2
G2881B - Ravenscrag Alberta Slip Celadon
G2890B - Randy's Red Original Cone 6 Glaze
G2894 - Ravenscrag Tenmoku #1
G2894A - Ravenscrag Tenmoku #2
G2908A - Alberta Slip Floating Blue
G2917 - Ravenscrag Floating Blue
G2926 - Perkins Clear
G2926A - Perkins Clear with Frit 3134
G2926B - Cone 6 Clear Glossy Base
G2926BL - G2926B Cone 6 Gloss Black
G2926J - G2926B Reduced COE (Li2O)
G2926S - G2926B Reduced COE (MgO)
G2931 - Worthington Cone 06-2 Clear
G2931F - Zero3 Ulexite Transparent Glaze
G2931G - Zero3 G Low Expansion Low Fire Clear
G2931H - Zero3 H High Expansion Variant
G2931K - Zero3 K Cone 03 Transparent Glaze
G2931L - Zero3 L Low Expansion Variant
G2931L2 - Zero3 L Low Expansion w/F-69
G2932 - Deb's Clear #1 Cone 04-02
G2932A - Deb's Clear #2
G2933 - Gerstley:PV Clay low fire clear
G2934 - Cone 6 Magnesia Matte Base
G2934A - High Dolomite-Testing glaze
G2934BL - G2934 85:15 Adjustable Matte Black
G2934J - G2934 with ZnO for Brown Stains
G2934J1 - G2934 (glossed using ZnO)
G2934Y - G2934 (lower-LOI)
G2934Y1 - G2934Y (Anti-Crawling)
G2934Y2 - G2934Y (Higher COE/Stony)
G2934Y3 - G2934 Super Durable
G2934Y4 - G2934 Super Durable #2
G2934Z - G2934Y Red Using F-69
G2936 - Ravenscrag Low Expansion Cone 6 Base
G2936B - Ravenscrag Low Expansion White Base 2
G2936C - Ravenscrag Original Cone 6 Base Glaze
G2938 - Wright's Water Blue Base
G2941A - Leach's Satin Clear Original
G2941C - Leach's Satin Clear - Craze fix
G3806 - Panama Blue Cone 6
G3806A - Panama Blue 2 - More clay, Copper Oxide
G3806B - Panama Blue 3 - Copper Carbonate
G3806C - Panama Cone 6 Adjustment 2015
G3806D - Panama c6 - Lower COE #1
G3806E - Panama c6 - Lower COE #2
G3806F - Panama c6 - Lower COE #3
G3806K - Panama c6 - Lower COE #7
G3806N - C6 Fluid Clear Final Recipe #10
G3808 - Cone 6 Bright Clear - Shaun Mollonga
G3808A - Cone 6 Bright Clear using Frits
G3813 - Campana Cone 6 Transparent Glaze
G3813B - Campana Clear Lower Expansion #2
G3813C - Campana Clear Low Expansion (no Spodumene)
G3814 - Low Zinc High Feldspar Fritless base
G3822 - Spectrum Clear 700 Dipping Glaze
G3834 - Tenmoku Cone 6
G3840 - Shino Trial Number 1
G3868 - Gold - Cone 6
G3868A - Gold Using Spodumene
G3868B - Gold Using Fusion Frit 493
G3868C - Gold Using Frit #2
G3875 - Tangerine 4 (Orange)
G3875B - Zinc Clear cone 6
G3875C - Tangerine + Orange Stain
G3879 - Cone 04+ UltraClear Glossy Base
G3879C - Cone 04 UltraClear Low-Expansion
G3879E - Cone 04+ UltraClear Glossy Base
G3879F1 - Cone 04+ UltraClear Glossy Base
G3888 - Kieth Davitt High-fluid-melt copper blue
G3892 - Val Cushing Satin White #71
G3903 - Alberta Slip + Frit FZ-16
G3904 - Original Recipe Using Frit 3124
G3904A - 3134 Mistake Recipe Fixed
G3909 - Ravenscrag Cone 10R Matte Blue
G3910 - Fritted version of G1947U #1
G3910A - Fritted version of G1947U #2
G3912A - Surface Tension White Tin
G3914A - Alberta Slip Gloss Black
G3918 - Red Mustard in G2571A Base #1
G3925 - Perfect Clear
G3925B - Perfect Clear Make-Over #1
G3926B - G2926B with Tin/Zircopax
G3926C - G2934 White Tin/Zircopax
G3933 - G2934:G2926B Oatmeal - Cone 6
G3933A - G2934:G2926B Oatmeal Cone 6
G3933E - G3933 Oatmeal Ravenscrag #2
G3933EF - G3933 Oatmeal Ravenscrag #4
G3933G1 - G3933 Oatmeal Alberta Slip + Li
G3939A - Cone 6 Oxidation Marbled Red
G3948 - Red Orange Glazy Original
G3948A - Iron Red Orange
G3955 - N505 Base Satin White - Opaque
G3956A - Bory1 Crystal Glaze for cone 6
G3966 - Cone 10R S2 - Luke Lindoe
G3971 - Lead Bisilicate Glaze
G3973 - Hilda Ross Rust
G4546 - Pattis Crystal Clear Cone 6
G4594 - 3B as a glaze
G4613 - Custer Feldspar Crackle Cone 10
G4613A - Minspar Crackle Cone 10
GA6-A - Oringal Alberta Slip Amber/Honey base
GA6-F - Alberta Slip Cone 6 Oatmeal
GR10-A - Ravenscrag Cone 10R Transparent Base
GR10-C - Ravenscrag Talc Matte
GR10-CW - Ravenscrag Cone 10R Talc Matte White
GR6-H - Ravenscrag Cone 6 Oatmeal
H0009 - 1945 MEDALTA FILTER CAKE
L2553B - Imco Carbondale Clay - C-Red
L2596E - H550 Casting Body #5
L2596F - H550 Casting Body #6
L2596G - H550 Casting Body #8
L2626 - Barnard Slip
L2950 - Hawthorn Fireclay #35
L3118A - RedArt:Ball Clay 40:60 Test
L3118J - Redart Grogged 10R Stoneware
L3127E - Boraq 1
L3127G - Boraq 2
L3127I - Boraq 3
L3127N - Boraq 5 #4 (available materials)
L3146A - Foundry Hill Creme+Nepheline
L3146B - New Foundry Hill Creme
L3146C - FHC + Kyanite
L3146D - FHC + Pyrax
L3164A - Cordierite Flameware - more bentonite, added grog
L3254 - OM #4 Ball Clay (50:50 raw:calcine)
L3320 - Cedar Heights Goldart clay
L3500 - Alberta Slip Original cone 6 base glaze
L3500G - Alberta Slip + Frit 3249
L3500H - Alberta Slip + Frit 3249 and Silica
L3523 - Cone 04 Gerstley Borate matte base
L3523A - Compare Boraq 5 #1 with GB in a glaze
L3523B - L3523 glaze using Boraq 5 L3127L
L3523C - L3523 glaze using Boraq 5 L3127M
L3523D - L3523 recipe using Boraq 5 L3127N
L3617 - Cornwall Stone substitute #2
L3619 - Cornwall Stone Average Analysis
L3660C - Flameware - Very High Pyrax with Molochite
L3660G - Pyrax/Kaolin Flameware
L3660P - Pyrax Flameware (low fire)
L3664A - PV CLAY Feb 2013 Shipment
L3673 - Laguna Barnard Slip Sub
L3685U1 - Zero3 Engobe Recipe
L3685Y - Cone 03 Terrastone 2 Engobe
L3685Z2 - Z2 White Cone 04 Engobe Base (no frit)
L3685Z3 - Z3 White Cone 04 Engobe (5% frit)
L3685Z5 - White Cone 04 Engobe for L4170B (3% frit)
L3685Z6 - Brown Engobe for Snow
L3685Z7 - Cone 04 Brown Engobe for Snow
L3685Z8 - White Cone 2 Engobe for L215, L210, L4170B (2% frit)
L3693E - Alumina Lining for Crucibles
L3693E1 - Zircon Lining for Crucibles
L3693H1 - Plastic Refractory Alumina Body H1
L3724L - Redart:Ball Clay 80:20 Test
L3724M1 - Redart Fritware #4
L3724M2 - Redart Fritware #5
L3724N - Redart Fritware #1
L3724N2 - Zero3 Stoneware
L3724P - Redart Fritware #2
L3728 - Cone 6 Dolomite Testing Glaze
L3778D - Cone 6 Translucent Grolleg Plastic
L3778D1 - Cone 6 Grolleg Pink/Blue Porcelains
L3778G - Cone 6 Translucent Grolleg Casting
L3798C - M340 Casting Body
L3798G - M340C Casting Body Revision 7
L3802E - Crystal Ice - Cone 10
L3802F - Crystal Ice - Cone 6 v1
L3806L - Panama c6 - Lower COE #8
L3840 - Diatomaceous Earth (Ant Killer)
L3868 - Craft Crank - From PotClays, UK
L3868A - Craft Crank - Base
L3868C - Craft Crank Clone 2
L3869 - Crank Industrial - From England
L3869A - Industrial Crank Base
L3894D - PV Calc Mix 4
L3906 - P300 Cone 6 Casting Body
L3911 - Bizen Clay
L3916 - Bizen Duplicate using Plainsman Materials
L3924C - Zero3 Porcelain - Experimental
L3924J - Zero4 Plastic Porcelain
L3924L - Zero4 Casting Porcelain
L3954B - Cone 6 White Engobe Recipe
L3954F - Cone 6 Black Engobe
L3954J - Black Cone 10 Whiteware Engobe Recipe
L3954N - Cone 10 Engobe for H550
L3954R - Super-White Engobe for Cone 6
L3954S2 - White Engobe (lower firing shrinkage)
L3972 - 98 Mix
L3977 - BGP Low Stoneware Body
L4001 - Super Kiln Wash
L4005D - M390 Casting Version 5
L4023F - Proposed H440 Casting Body #5
L4028 - G2571A Rutile Bamboo
L4053B - Cone 6 Black Clay Body - Type 1
L4068 - Barnard Chemical Substitute
L4115J3 - L211 Stnwre 3D:OM4:NS
L4115L2 - L211 3D:OM4:NS:Talc 42 mesh
L4115L2a - L211 3D:OM4:NS:Talc 80 mesh
L4158 - Cimtalc 15 Talc lab test
L4159 - Cimtuff 9115 Talc lab test
L4163 - Red Art Cone 1 Clay Body
L4168G5 - H440C (concentrate) #5
L4168G9 - New H440 Functional Proposal #8
L4170 - L215 Terra Cotta Casting #1
L4170B - Terra Cotta Casting #2
L4170F - Terra Cotta Casting #3
L4208C - MNS Cone 6 Fine Stoneware
L4208D - 3B +200# particles sieved out
L4217G - M370-like Cone 6 Faster Casting
L4227 - Plus Clay
L4228 - Fimo Clay
L4237 - Redart Tile Body
L4239 - H550 Casting Body #7
L4244 - BGP Clay:Flyash F 50:50 Mix
L4244A - Flyash F:Bentonite 10:90
L4245 - LaFarge Fly Ash F:Bentonite 95:5 Mix
L4245F - Fly Ash F:Bentonite:BallClay 80:10:10
L4246 - A2 +200# particles sieved out
L4247 - A3 +200# particles sieved out
L4248 - Old Hickory M23 Ball Clay
L4249 - 3D +200# particles sieved out
L4249A - 3D MNS 325 Mesh
L4249B - 3D 100 mesh
L4264 - Raku Crackle Glaze Base - Frit 3110
L4264A - Raku Glaze Base #1
L4264B - Raku Glaze Base #2
L4264C - Raku Glaze Base #3
L4264D - Raku Glaze Base #4
L4273 - G3806N1 + 2% Zircopax
L4280 - L215 : M390 Mix for Cone 1 Stoneware
L4287 - Midfield Clay Yukon
L4287A - Catchment Clay Yukon
L4292 - Monte Marte Air Hardening Clay
L4293 - DAS Air Drying Clay
L4294 - Sculpey PE08 Oven Bake Clay
L4398 - Ravenscrag Cone 6 Raspberry
L4404A - Refractory Casting Slip
L4404B - Plastic Refractory (heavy duty)
L4404C - Refractory Plastic (low expansion)
L4404D - Refractory Casting (low expansion)
L4410L - L213 NS:Dolo 30:20
L4410P - L213 40:10 Dolo/NS
L4421 - Seed pelleting clay and binder
L4441A - Minspar
L4441B - Minspar Calculated Substitute
L4453C - 3D:A2 Body Base H550 Blend
L4458 - Lithium Flameware Test
L4482B - Alumina Wadding #2
L4484D - 2018 3B+6% 6666 at 100#
L4498 - Low Expansion Super White Cone 6 Fritware
L4498A - Low Expansion Fritware Casting
L4530 - Carbondale M390 #1
L4530A - Carbondale M390 #2
L4532A - Pyrometric cone pressing body #2
L4532B - Cone pressing body #3
L4532D - Cone pressing body #5
L4532F - Cone 5 Cone-casting v.1
L4543 - Firebrick & kiln post/shelf clay - v1.0
L4543B - Firebrick & kiln post clay v2.0
L4543C - Refractory kiln post clay v4.0
L4557 - Volumetric Screw Feeder Design - ESP32 based
L4558 - M390 Casting (M370+C-Red)
L4558A - M390 Cone 6 C-Red Casting #1
L4558B - M390 Cone 6 C-Red Casting #2
L4567 - Cat Litter
L4575 - SIAL Refractory Slip
L4575A - SIAL refractory slip Duplicate
L4588 - Red NZK Cone 6 Porcelain
L4597 - Luke Lindoe Fired Samples
L4599 - Slip for Slipware
L4599A - Slip for Slipware - #5 Ball Clay
L4608 - Kyanite Bisque-Fix, Kiln-Patch
L4655 - Titanium Dioxide in GA6-C
L4655A - GA6-C Titanium + Iron
L4655B - GA6-C Lower Thermal Expansion
L4696 - Cordierite Flameware
L4697 - Flameware body from French mfgr
L4705A - GA6-C Using Frit 3195 and Titanium
L4768D - Cone 6 Black Casting Body - Type 2
L4768E - Cone 6 Black Casting Body - Type 3.1
L4768H - Cone 6 Black Casting Body - Type 3.3
L4807 - M370-like Super-Fast Casting Porcelain
LCHUN - Lindoe Chun cone 10R
MRG6B - G2850A Ravenscrag Cone 6 Light Blue
MRG6C - Ravenscrag Cone 6 White Glossy
MRG6E - G2850P Ravenscrag Cone 6 Raspberry
MRG6G - G2851H Ravenscrag Cone 6 Light Blue Matte
P4738A - 98 BGP RETEST
P4808 - 45D
P6385 - M2 ST
P6821 - L215 Production Run - Mar 2020
P7088 - H440
PC-32 - Amaco Glaze: PC-32 Albany Brown

G2928C - Ravenscrag Silky Matte for Cone 6

Modified: 2022-01-30 15:59:15

Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

Material Amount Percent
Ferro Frit 313411.0010.4
Talc8.007.6
Ravenscrag Slip60.0056.9
Nepheline Syenite13.0012.3
Wollastonite1.501.4
Calcined Kaolin12.0011.4
Added
Tin Oxide5.004.74
110.50 100

Notes

This works well on Plainsman M340, but especially on a whiteware like M370. Produces an ivory white with some fleck. The surface is very silky, reminiscent of a cone 10 dolomite matte. Its matteness is adjustable by varying the amount of calcined kaolin (or simply blending in a glossy recipe to shine it up a little). The mechanism of the matteness is high MgO in a boron base of low Si:Al ratio.

Do not use regular kaolin, the glaze will shrink too much during drying.
Use enough water in the slurry so it flows well, it will apply very evenly without drips. If there is not enough water and the slurry is too creamy, it will crack during drying and crawl during firing. Calcine part of the Ravenscrag to reduce the shrinkage if needed.

The tin oxide is included to whiten and opacify the glaze, if you remove it the color will be quite a bit darker, especially on darker clay bodies (Ravenscrag contains some iron). The 1.5 wollastonite is a remnant of how this glaze was created; it started as Moores Matte, a well-known Gerstley Borate-based matte recipe. We first reformulated it to substitute the GB for a frit (while maintaining the same chemistry) and then incorporated Ravenscrag Slip to supply as much of the rest of the chemistry as possible. A further adjustment was made to make the surface more silky. The silky matte G2934 followed this, it being a cleaner, whiter variant having no Ravenscrag but the same fired surface.

Since this has some iron, colouring it with stains could produce more muddied colours than you might want. Consider using the G2934 base instead if needed.

Related Information

G2928C does not work well on dark-burning bodies


This picture has its own page with more detail, click here to see it.

Plainsman M390 (right) generates gases of decomposition (from its LOI) at a time when the G2926C glaze is unable to handle them (thus they leave pinholes and bubbles). The same glaze is good on M340 (a buff stoneware on the left), but it is even better on a porcelain.

A functional matte liner glaze is possible - with care.


This picture has its own page with more detail, click here to see it.

Ravenscrag G2928C matte liner glaze is on the insides of these mugs. Like our G2934 recipe, this matte glaze needs to be fired to a real cone 6 and fired in the C6DHSC drop and hold and then slow-cooled schedule. If cooled too slowly the surface could be too matte would be subject to cutlery marking (especially on the inside bottoms). If cooled too quickly it will be too glossy. When firings cool slowly just because they are tightly packed the degree of matteness can be tuned by blending in just enough glossy glaze to make the surface smooth enough to be functional while still matte enough to be attractive to the eye and the touch.

Ravenscrag based silky MgO matte at cone 6


This picture has its own page with more detail, click here to see it.

Cone 6 G2928C Ravenscrag Silky Matte on Plainsman M340 (left) and M370 (right). The inside of the M370 mug is a transparent glossy. This recipe produces a silky ivory-coloured surface of very good quality.

Comparing two glazes having different mechanisms for their matteness


This picture has its own page with more detail, click here to see it.

These are two cone 6 matte glazes (shown side by side in an account at Insight-live). G1214Z is a calcia matte, it has a high silica:alumina ratio. It crystallizes during cooling to make the matte effect. Melt fluidity is needed for that and this GLFL test shows that it certainly has that. The degree of matteness is adjustable by tuning the SiO2 content. The G2928C is a magnesia matte, it has high MgO and produces the classic silky micro-wrinkled the surface. Its matteness is adjustable by trimming the calcined kaolin. CaO is a standard oxide that is in almost all glazes, 0.4 is not high for it. But much less MgO is needed for it to make a matte. The G2928C also has 5% tin, if that was not there it would be darker than the other one because Ravenscrag Slip has some iron. This glaze actually has texture like a dolomite matte at cone 10R, it is great. And it has wonderful application properties. And it does not craze, on Plainsman M370 (it even survived a 300F-to-ice water IWCT test). This looks like it could be a great liner glaze.

This surprised me about calcia matte glazes:

Most are highly melt fluid.


This picture has its own page with more detail, click here to see it.

Unfortunately, many matte glazes are such simply because they are not melted enough. That is not the case with cone 6 G1214Z tested here. When applied as a thin layer on pottery, it seems normal. But this GLFL test demonstrates that it fires highly melt fluid, much more than one might expect from a matte glaze. A quick look at its oxide chemistry reveals the reason: It is a calcia matte. It has high CaO, so as the melt cools, it combines with SiO2 and even Al2O3 to form calcium silicate crystals (instead of staying in the glass).

What is the G2928C? That is Ravenscrag cone 6 Tri-Matte; it employs three matteness mechanisms: High CaO, MgO and Al2O3. It contains significant Tin Oxide (thus the white color).

Links

Recipes GR10-C - Ravenscrag Cone 10R Silky Talc Matte
Just Ravenscrag Slip plus 10% talc produces a visually variegated surface that feels silky and looks stunning!
Recipes G2934 - Matte Glaze Base for Cone 6
A base MgO matte glaze recipe fires to a hard utilitarian surface and has very good working properties. Blend in the glossy if it is too matte.
Recipes G1214Z1 - Cone 6 Silky CaO matte base glaze
This glaze was born as a demonstration of how to use chemistry to convert a glossy cone 6 glaze into a matte.
Glossary Matte Glaze
Random material mixes that melt well overwhelmingly want to be glossy, creating a matte glaze that is also functional is not an easy task.
Glossary Magnesia Matte
Magnesia matte ceramic glazes are “microstructure mattes” while calcia mattes are “crystal mattes”. They have a micro-wrinkle surface that forms from a high viscosity melt and microscopic phase separation, both of which prevent levelling on freezi
Media How I Formulated G2934 Cone 6 Silky MgO Matte Glaze Using Insight-Live
I will show you how found a recipe on Facebook, assessed it, substituted my own materials, tested it, adjusted it.
Typecodes Medium Temperature Glaze Recipes
Normally fired at cone 5-7 in electric kilns.
Typecodes Matte Glaze Recipes
Much less common that glossy glazes, normally have stricter firing requirements.
Firing Schedules Plainsman Cone 6 Electric Standard
Used in the Plainsman lab to fire clay test bars in our small kilns

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

XML to Paste Into Insight-live

<?xml version="1.0"?>
<recipes version="1.0" encoding="UTF-8">
<recipe name="Ravenscrag Silky Matte for Cone 6" keywords="Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com." id="119" date="2022-01-30" codenum="G2928C">
<recipelines>
<recipeline material="Ferro Frit 3134" amount="11.000"/>
<recipeline material="Talc" amount="8.000"/>
<recipeline material="Ravenscrag Slip" amount="60.000"/>
<recipeline material="Nepheline Syenite" amount="13.000"/>
<recipeline material="Wollastonite" amount="1.500"/>
<recipeline material="Calcined Kaolin" amount="12.000"/>
<recipeline material="Tin Oxide" amount="5.000" added="1"/>
<url url="https://backup.digitalfire.com/recipe/119" descrip="https://backup.digitalfire.com/recipe/119"/>
</recipelines>
<urls/>
</recipe>
</recipes>
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy