Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Sodium Azide Toxicology

Introduction

There are potters who suggest the use of Sodium Azide as a biocide in slips and gums.
"Depending on time, temperature, pH, gum can be attacked by microbes or molds. If this happens store in a cooler place, make smaller batches, adjust the pH to make a less friendly environment, or add an antiseptic i.e. NaN3
I put sodium azide in my CMC solutions - just a tiny pinch, less than 0.5% stops bacteria cold turkey". (Clayart, 2004)
We disagree with the use of this chemical for the following reasons :

Sodium azide :

An azide is a compound of hydrogen or a metal ion and the monovalent -N3 radical.
Sodium azide is used in protection airbags of cars and this use has increased a lot its production. In small amounts it is used in biology labs as an antimicrobial in reagents.

I-Experimental Toxicology :

In animals it is a poison by ingestion, skin contact, intraperitoneal, intraveinous, and subcutaneous routes.

II-Human Toxicology :

The lowest toxic dose by ingestion is 5 mg.

A-Routes of Entry :

-Ingestion,
-Inhalation,
-Skin

B-Ingestion :

1-Peripheral vasodilatation :

rapidly causing a drop in the blood pressure :
-vertigo,
-a tendancy to loose consciousness,
-palpitations,
-sweating,
-headaches

2-Severe cases :

Cardiovascular collapsus.

3-Cardiac Ischaemic Symptoms :

If the amount ingested is large, cardiac ischaemic symptoms and signs may occur ( 80 mg).

4-Severe Acute Intoxication (Suicide) :

-coma (brain oedema),
-collapsus,
-cardiac arythmias,
-metabolic acidosis,
-respiratory depression,
-pulmonary oedema.

Treatment :

There is no known treatment.

C-Inhalation :

In a study among workers exposed to airborne sodium azide, most suffered from :
-headaches,
-periods of hypotension
-palpitations.

Two workers exposed to large amounts of this chemical suffered from :
-cough,
-nausea,
-vomiting,
-headaches,
-vertigo,
-hypotension;
- RADS, Reactive Airways Dysfonction Syndrome, an asthma-like condition (delayed reaction).

Mutagenesis :

Human mutation data reported.

Hazardous Reactions :

Reacts violently with many chemicals.
Reacts with heavy metals to form dangerously explosive heavy metal azides, a particular problem in laboratory equipment and drain traps Sodium azide " per se " can be an explosion danger, following a shock or when heated rapidly

Thermal Decomposition :

When heated to decomposition it emits very toxic fumes of NOx,
and Na2O.

Azides :

Variable Toxicity.
Many azides are poisonous, and cause a fall in blood pressure, and some inhibit enzyme action, thus resembling nitrites and cyanides.
All azide salts and the acid are unstable and some decompose explosively, altough lead azide, which is one of the most important azides, is not very sensitive.

Hazardous Decomposition :
When heated to decomposition they emit highly toxic fumes.

Explosiveness :
Schock and heat will explode them.
If exposed to CS2, they form violently explosive salts.

For more pertaining information on micro-organisms and ceramic material, go to :

http://perso.wanadoo.fr/smart2000/bacteries.htm
or
http://ceramic-materials.com/cermat/area.php?areaid=8&find=micro-organisms

Reference:
1-Toxicologie Industrielle et Intoxications Professionnelles, Lawerys R.R.
2-Sax's Dangerous Properties of Industrial Materials, Lewis R.
 

By Edouard Bastarache

Related Information

Links

Materials Tektamer 38 Biocide
Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy