Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Man-Made Vitreous Fibers Safety Update

A report we received May 2021 from NAIMA (North American Insulation Manufacturers Association) giving a current US perspective from the industry. A link to the PDF version of this document (with references) is provided below.

The extensive epidemiology data on MMVF manufacturing workers comprise the best and most conclusive information on the safety of mineral wool and other MMVFs and take precedence over any in vitro data.  These data have not shown any evidence of chronic disease, malignant or nonmalignant, directly attributable to MMVF exposure.

When the International Agency for Research on Cancer (“IARC”) evaluated all the epidemiology data in its 2002 review, it concluded that the epidemiology data were inadequate to suggest any adverse effect. On human carcinogenicity data, the IARC experts concluded that:

Results from the most recent cohort and nested case-control studies of US workers exposed to glass wool and continuous glass filament and of European workers exposed to rock (stone) and slag wool have not provided consistent evidence of an association between exposure to fibres and risk for lung cancer or mesothelioma.

These conclusions are based on an unusually robust body of data from many countries – a European cohort study, an American cohort study, a Canadian cohort study, a Swedish cohort study, cohort studies narrowly focused on certain population segments or single production facilities, and case-control studies in England, Europe, the United States, and others.  In Europe, the epidemiological studies were conducted under the direction of P. Bofetta, IARC, Lyon, France, with the associated industrial hygiene being carried out by the Institute of Occupational Medicine (“IOM”), Edinburgh.  The epidemiological research in the United States was undertaken at the University of Pittsburgh in the Department of Biostatistics and the Center for Environmental Epidemiology with Gary Marsh as Principal Investigator.  The industrial hygiene program was also conducted at the same University in the Department of Industrial and Environmental Health Sciences.  To this day, these two studies – Europe and the United States – separately are among the largest occupational cohort studies ever undertaken.  Based on this evidence, the IARC experts concluded that “[t]here is inadequate evidence in humans for the carcinogenicity” of rock wool and of other MMVF fiber types.

Specifically, IARC found the U.S. MMVF cohort showed no association with “duration of exposure or with time since first exposure.”  Moreover, IARC found that standardized mortality ratios (“SMR”) were no longer elevated when indirect adjustment for smoking was made.  The nested case-controlled study for rock wool showed no association between respiratory cancer and estimated cumulative exposure to respirable fibers, with or without adjustment for possible confounding by smoking or other occupational exposures.  IARC concluded that the “results from these studies provide no evidence of an increased risk for pleural mesotheliomas or any other tumours.”  The extensive European epidemiology studies included a case-control study with “detailed information on exposure to fibres, individual smoking habits and potential occupational confounders, no increased risk of lung cancer with increasing fibre exposure was reported.”

In its Toxicological Profile for Synthetic Vitreous Fibers, the Agency for Toxic Substances and Disease Registry (“ATSDR”), after extensive review, reached the same conclusion as did IARC on the epidemiological evidence:

These comprehensive epidemiological studies have already received exacting scrutiny from the world’s foremost experts.

Since the release of the 2002 IARC Monograph, numerous epidemiological studies have evaluated the association between MMVF exposure and respiratory system cancer, including cancers of the lung, bronchus, larynx, and trachea. Dr. Marsh, et al., conducted a systematic review and meta-analysis of epidemiological literature evaluating the association between exposure to MMVF and respiratory system cancers in 2019. The authors of the review and meta-analysis concluded that the 2002 IARC Group 3 classification of insulation glass wool, rock wool, and slag wool remains valid.

The epidemiology study results, relied upon by IARC, did not find evidence that MMVF exposures were associated with cancer in manufacturing workers.  As high quality epidemiology studies of workers are always the most significant evidence of the effect or lack of effect of any exposure, these studies provide powerful evidence that MMVFs among manufacturing workers were not associated with disease.

EXTENSIVE EVIDENCE FROM ANIMAL STUDIES CONFIRMS NO CANCER HAZARD FROM INSULATION MMVF

Extensive evidence from many studies in multiple animal species confirms that the MMVF in insulation products, both in products from decades ago and in use today, do not present a cancer hazard by inhalation. The animal studies performed in the 1990s, including long term inhalation studies that last for the entire life of the test animals, are well summarized in several peer-reviewed journal articles. In its 2002 Monograph, IARC relied heavily on these animal studies in removing insulation MMVF from its list of Group 2B possible carcinogens.

THERE IS A DISTINCT DIFFERENCE BETWEEN ASBESTOS AND SYNTHETIC VITREOUS FIBERS

Fiber glass and mineral wool fibers are distinctly different from asbestos. The ATSDR provided a detailed discussion on the differences between fiber glass insulation fibers and asbestos in its Toxicological Profile for Synthetic Vitreous Fibers:

Thus, MMVF and asbestos are chemically, morphologically, and toxicologically distinct. While they may have some superficial similarities, well-established science and hazard classification decisions from authoritative scientific bodies confirm that asbestos presents serious health hazards while insulation MMVF does not.

EXPOSURES ARE LOW

Based on review of various exposure studies, IARC concluded that concentrations of airborne fibers measured during the production of glass and slag and/or rock (stone) wool are generally low (below 1 fiber/cm3). ATSDR concluded that “The airborne levels of synthetic vitreous fibers have been shown to be higher under occupational settings as compared to ambient air levels, and thus, occupational exposure is far greater than the exposure for the general population.” Based on various exposure studies and the NAIMA database, ATSDR concluded that exposures were consistently below 1 f/cc. Testing of indoor exposures also demonstrates that exposures are very low. Exposure monitoring conducted near fiber glass manufacturing facilities showed low exposures, too.


By Tony Hansen
Follow me on

Related Information

Links

Hazards Man-Made Vitreous Fibers (MMVF) Toxicology
Satety and hazard info of aluminum silicate ceramic fiber materials (e.g. fibre glass, mineral wood, refractory ceramic fibre).
URLs https://digitalfire.com/4sight/datasheets/MMVF-Toxicology-2021.pdf
Detailed MMFV Epidemiology Data as of 2021
From NAIMA (North American Insulation Manufacturers Association).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy