Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Lithium Toxicology


There is no described professional intoxication from the use of this element. Data on its toxicity to man comes from its use as the treatment of choice in manic-depressive states, and from suicidal attempts.



Treatment with lithium carbonate may cause the following:



Moderate side-effects

Diarrhea, nausea,

Feeling of thirst,

Vision troubles,

Tremors of the hands.

More severe side-effects

Memory disorders, tremors, muscular fasciculations,

Hyperactive tendon reflexes, dysarthria, giddiness.

Severe intoxication leads to convulsions and coma, which can be hyperosmolar.

Prolonged treatment

Interstitial nephritis, incomplete distal tubular acidosis,

Hyperparathyroidism (hypercalcemia),

Disturbances of the glucose metabolism, obesity,

Goiter, hypothyroidism,

Neutrophilia,

Various cutaneous lesions (psoriasis, acne, folliculitis, alopecia, etc.)

Toxic manifestations may occur when the serum concentration exceeds 10.4mg/L. A concentration higher than 25mg/L justifies treatment by dialysis.(1)



The toxic and therapeutic blood levels are very close, so any activity leading to loosing much body water may switch a patient taking lithium carbonate form the therapeutic to the toxic zone, as in sweating excessively in melting departments of steel mills.



Also, many anti-inflammatory drugs raise lithium blood levels of patients and may cause intoxication, one major offender being ibuprofen ( Motrin, Advil). It is important to remember this name because it may be sold without a prescription.



Other possible offenders are ketorolac (Toradol), diclofenac (Voltaren), indomethacin (Indocid), naproxen (Naprosyn), fenoprofen (Nalfon), celexobib (Celebrex), rofecoxib (Vioxx). (2)



There is no such thing as a single case of lithium intoxication described in the pertaining literature from the use of it in glaze making or from the use of ceramic wares covered by lithium-containing glazes.



The only lithium compound that is reported as a severe hazard is lithium hydride (LiH), which is used as a condensing agent in chemical synthesis with acid esters and ketones, as a dessicant (a reducing agent), and as a hydrogen source.



The hydride is a severe irritant to skin and mucous membranes because it becomes lithium hydroxide when in contact with the moisture of these structures.(3)



So, if you do not use the hydride, have a nice day.



References

Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R. last edition.

Sylvie Dumaine, pharmacist, Sorel-Tracy, Quebec, Canada (2002)

Occupational Medicine, Zenz Carl, last edition.


By Edouard Bastarache

Related Information

Links

Materials Lithium Carbonate
A powerful melter very valuable in ceramic glazes. It is 40% Li2O and has an LOI of 60% (lost as CO2 on firing). This material in now incredibly expensive.
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Lepidolite
Hazards Lithium Carbonate Toxicity
Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy