Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Gallium Oxide Toxicology

Introduction

CAS # :12024-21-4
Transition metal oxide

Toxicology

Exists as a white powder.

Oral LD50 : 10000 mg/kg (mus), therefore low toxicity by ingestion.

Rats exposed by inhalation to gallium oxide 2 hours/day for 20 days developed severe pulmonary inflammation (alveolitis) evolving to fibrosis.

Gallium and gallium compounds may cause metallic taste, dermatitis and depression of the bone marrow function. Large doses may cause hemorrhagic + nephritis.

May cause eye irritation.

May cause skin irritation.

May cause respiratory irritation.

May cause irritation in digestive tract.

None

First Aid Measures

Flush eyes with warm water for 15 minutes, occasionally lifting the upper and lower eyelids. If irritation persists, seek medical attention.

Wash with soap and water. If irritation persists, seek medical attention.

Take deep breaths of fresh air and avoid further inhalation of the material. If irritation persists, seek medical attention.

Drink 2 cups of water and induce vomiting. Seek immediate medical attention

Fire Fighting Measures

Use water, carbon dioxide, dry chemical extinguishing agents, dry sand or dry ground dolomite

Wear an approved self-contained breathing apparatus and full protective clothing.

Not Applicable

Accidental Release Measures

Stay away from spill so as to avoid airborne dust. Exposure concerns are limited to inhalation and, in the case of a very large all-surrounding spill, suffocation.

Spill should be contained if it can be done without risk.

Do not dispose of spill by dumping into public sewer or any other unauthorized waste treatment system. Spill should be swept up and properly prepared for disposal.

Should spilt material enter an unauthorized waste treatment system, contact the local authorities.

Handling and Storage

None

Use appropriate respiratory protection when exposure exceeds the established limits. Wash thoroughly after handling.

Keep containers tightly closed and in cool, dry, well-ventilated areas.

Exposure Controls/Personal Protection

Prevent eating, drinking, tobacco usage and cosmetic application in areas where there is a potential for exposure to the material. Always wash thoroughly after handling.

To avoid eye contact, wear safety glasses with side shields or chemical goggles.

To avoid skin contact, wear rubber gloves, boots, long-sleeved shirts, long-pants and head covering.

To avoid inhalation wear dust mask or self-contained respiratory device.

Add ventilation capacity if current environment cannot maintain airborne concentrations below the established exposure limit.

None

Stability and Reactivity

Stable under normal conditions of storage and handling.

Will not occur.

Not Applicable

Not Applicable

When heated to decomposition it emits toxic vapors of Ga.

Skin Sensitization

No information is known.

Mutagenicity Data

No information is known.

Reproductive/Teratology Data

No information is known.

Carcinogenicity Data

No information is known.

Ecological Information

Eco-acute Toxicity

Acute toxicity is considered unlikely because of the existence of similar compounds in nature.

References

  1. Occupational Medicine,Carl Zenz, last edition.
  2. Clinical Environmental Health and Toxic Exposures, Sullivan & Krieger; last edition.
  3. Sax039;s Dangerous Properties of Industrial Materials, Lewis C., last edition.
  4. Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R.R. last edition.
  5. Chemical Hazards of the Workplace, Proctor & Hughes, 4th edition
  6. Répertoire Toxicologique de la CSST du Quebec.
  7. Pacific Industrial Development Corp, MSDS, Gallium Oxide, January 2002.

By Edouard Bastarache

Related Information

Links

Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy