Ferro Frit 3124
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature glossy glaze. |
| Materials |
Frit FA-233-2 (approx)
|
| Materials |
Ferro Frit CC-279-3 (approx)
|
| Materials |
Ferro Frit CC-274
|
| Materials |
Ferro Frit CC-272
|
| Materials |
Ferro Frit CC-263
|
| Materials |
Ferro Frit CC-250
|
| Materials |
Ferro Frit 5301
|
| Materials |
Ferro Frit 3292
|
| Materials |
Ferro Frit 3278
|
| Materials |
Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes. |
| Materials |
Ferro Frit 3270
|
| Materials |
Ferro Frit 3269
|
| Materials |
Ferro Frit 3195
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature semi-glossy glaze. |
| Materials |
Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry. |
| Materials |
Ferro Frit FB-276-P-2 (approx)
|