80-250C (176-482F) | 80-250C (176-482F) | 120C (248F) | 150C (302F) | 180C (356F) | 185C (365F) | 200-450C (392-842F) | 200-1000C (392-1832F) | 200C (392F) | 210-280C (410-536F) | 260C (500F) | 290C (554F) | 300C (572F) | 300-330C (572-626F) | 300C (572F) | 370-700C (698-1292F) | 370C (698F) | 400C (752F) | 425-650C (797-1202F) | 450-650C (842-1202F) | 470-1200C (878-2192F) | 500-600C (932-1112F) | 512C (953F) | | 650-900C (1202-1652F) | 750-850C (1382-1562F) | 750-1000C (1382-1832F) | 760C (1400F) | 760C (1400F) | 787C (1448F) | 800-1100C (1472-2012F) | 815C (1499F) | 815C (1499F) | 843C (1549F) | 850C (1562F) | 850-950C (1562-1742F) | 850C (1562F) | 870-900C (1598-1652F) | 871C (1599F) | 900C (1652F) | 900-1000C (1652-1832F) | 900C (1652F) | 926C (1698F) | 932C (1709F) | 950-1050C (1742-1922F) | 954C (1749F) | 980C (1796F) | 982C (1799F) | 990C (1814F) | 1025C (1877F) | 1025-1325C (1877-2417F) | 1050-1200C (1922-2192F) | 1050C (1922F) | 1065-1120C (1949-2048F) | 1082C (1979F) | 1100-1450C (2012-2642F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1300C (2372F) | 1325C (2417F) | 1330C (2426F) | 1360C (2480F) | 1418-1428C (2584-2602F) | 1420C (2588F) | 1550C (2822F) | 1565C (2849F) | 1650C (3002F) | 1785C (3245F) | 1990C (3614F) | 2300C (4172F) | 2320C (4208F)

540-600C (1004-1112F)

Quartz inversion (alpha-beta)

This term refers to an abrupt change in volume that occurs in quartz crystals when they are heated from the room temperature stable alpha phase to the beta crystal phase that exists above a theoretical temperature of 573C. It is referred to as an inversion because the process is reversed when the temperature falls back below 573C (although the reversal expansion curve is not identical to the heatup one). Since the change occurs across a narrow range of temperatures, ware will crack if there are significant temperature gradients within it. For example, if one side of a piece is at 573 and the other at 600, then as the piece cools further the volume change will move horizontally across it and could start a crack at the first weakness it encounters. The range we indicate for quartz inversion recognizes the fact that kiln gradients almost always exist and that quartz inversion does not happen at one specific temperature as is often suggested (the curve of temperature vs expansion is simply much steeper across a narrow range than it is outside that range, about 50 degrees).

Quartz inversion can be beneficial because it can put the glaze under compression and thus prevent crazing.

Related Information

Links

Materials #1 Q-Rok
URLs http://en.wikipedia.org/wiki/Quartz_inversion
Wikipedia quartz inversion
Glossary Cristobalite Inversion
In ceramics, cristobalite is a form (polymorph) of silica. During firing quartz particles in porcelain can convert to cristobalite. This has implications on the thermal expansion of the fired matrix.
Glossary Quartz Inversion
In ceramics, this refers to the sudden volume change in crystalline quartz particles experience as they pass up and down a temperature window centering on 573C.
Temperatures Cristobalite inversion (alpha/beta) (210-280)
Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy