80-250C (176-482F) | 80-250C (176-482F) | 120C (248F) | 150C (302F) | 180C (356F) | 185C (365F) | 200-450C (392-842F) | 200-1000C (392-1832F) | 200C (392F) | 210-280C (410-536F) | 260C (500F) | 290C (554F) | 300C (572F) | 300-330C (572-626F) | 300C (572F) | 370-700C (698-1292F) | 370C (698F) | 400C (752F) | 425-650C (797-1202F) | 450-650C (842-1202F) | 470-1200C (878-2192F) | | 512C (953F) | 540-600C (1004-1112F) | 650-900C (1202-1652F) | 750-850C (1382-1562F) | 750-1000C (1382-1832F) | 760C (1400F) | 760C (1400F) | 787C (1448F) | 800-1100C (1472-2012F) | 815C (1499F) | 815C (1499F) | 843C (1549F) | 850C (1562F) | 850-950C (1562-1742F) | 850C (1562F) | 870-900C (1598-1652F) | 871C (1599F) | 900C (1652F) | 900-1000C (1652-1832F) | 900C (1652F) | 926C (1698F) | 932C (1709F) | 950-1050C (1742-1922F) | 954C (1749F) | 980C (1796F) | 982C (1799F) | 990C (1814F) | 1025C (1877F) | 1025-1325C (1877-2417F) | 1050-1200C (1922-2192F) | 1050C (1922F) | 1065-1120C (1949-2048F) | 1082C (1979F) | 1100-1450C (2012-2642F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1300C (2372F) | 1325C (2417F) | 1330C (2426F) | 1360C (2480F) | 1418-1428C (2584-2602F) | 1420C (2588F) | 1550C (2822F) | 1565C (2849F) | 1650C (3002F) | 1785C (3245F) | 1990C (3614F) | 2300C (4172F) | 2320C (4208F)

500-600C (932-1112F)

Magnesite decomposition

The process of removing the CO2 from magnesite to produce light magnesium carbonate is often called magnesite decarbonization. There is variation in the temperature ranges given for this phenomenon by different sources (e.g. some say 550-600C).

Related Information

Links

Materials Magnesite

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy