80-250C (176-482F) | 80-250C (176-482F) | 120C (248F) | 150C (302F) | 180C (356F) | 185C (365F) | 200-450C (392-842F) | 200-1000C (392-1832F) | 200C (392F) | 210-280C (410-536F) | 260C (500F) | 290C (554F) | 300C (572F) | 300-330C (572-626F) | 300C (572F) | 370-700C (698-1292F) | 370C (698F) | 400C (752F) | | 450-650C (842-1202F) | 470-1200C (878-2192F) | 500-600C (932-1112F) | 512C (953F) | 540-600C (1004-1112F) | 650-900C (1202-1652F) | 750-850C (1382-1562F) | 750-1000C (1382-1832F) | 760C (1400F) | 760C (1400F) | 787C (1448F) | 800-1100C (1472-2012F) | 815C (1499F) | 815C (1499F) | 843C (1549F) | 850C (1562F) | 850-950C (1562-1742F) | 850C (1562F) | 870-900C (1598-1652F) | 871C (1599F) | 900C (1652F) | 900-1000C (1652-1832F) | 900C (1652F) | 926C (1698F) | 932C (1709F) | 950-1050C (1742-1922F) | 954C (1749F) | 980C (1796F) | 982C (1799F) | 990C (1814F) | 1025C (1877F) | 1025-1325C (1877-2417F) | 1050-1200C (1922-2192F) | 1050C (1922F) | 1065-1120C (1949-2048F) | 1082C (1979F) | 1100-1450C (2012-2642F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1300C (2372F) | 1325C (2417F) | 1330C (2426F) | 1360C (2480F) | 1418-1428C (2584-2602F) | 1420C (2588F) | 1550C (2822F) | 1565C (2849F) | 1650C (3002F) | 1785C (3245F) | 1990C (3614F) | 2300C (4172F) | 2320C (4208F)

425-650C (797-1202F)

Sulfur evolution

This happens on first fire for many bodies. Sulfur is an impurity in many ball clays and related stoneware and earthenware raw clays, it occurs as calcium sulfate (selenite, the same mineralogy as plaster). Different sources indicate wider and narrower ranges for this, it is difficult to establish exactly.

Related Information

Links

Hazards Sulfur Dioxide Toxicity
This gas can be produced when clays are fired in a kiln. What can you do?
URLs http://en.wikipedia.org/wiki/Sulfur
Sulfur at Wikipedia
Minerals Selenite
A transparent crystal form of the mineral gypsum. This can occur in clays and is the cause of efflor

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy