80-250C (176-482F) | 80-250C (176-482F) | 120C (248F) | 150C (302F) | 180C (356F) | 185C (365F) | 200-450C (392-842F) | 200-1000C (392-1832F) | 200C (392F) | 210-280C (410-536F) | 260C (500F) | 290C (554F) | 300C (572F) | 300-330C (572-626F) | 300C (572F) | 370-700C (698-1292F) | 370C (698F) | 400C (752F) | 425-650C (797-1202F) | 450-650C (842-1202F) | 470-1200C (878-2192F) | 500-600C (932-1112F) | 512C (953F) | 540-600C (1004-1112F) | 650-900C (1202-1652F) | 750-850C (1382-1562F) | 750-1000C (1382-1832F) | 760C (1400F) | 760C (1400F) | 787C (1448F) | 800-1100C (1472-2012F) | 815C (1499F) | 815C (1499F) | 843C (1549F) | 850C (1562F) | 850-950C (1562-1742F) | 850C (1562F) | 870-900C (1598-1652F) | 871C (1599F) | 900C (1652F) | 900-1000C (1652-1832F) | 900C (1652F) | 926C (1698F) | 932C (1709F) | 950-1050C (1742-1922F) | 954C (1749F) | 980C (1796F) | 982C (1799F) | 990C (1814F) | 1025C (1877F) | 1025-1325C (1877-2417F) | 1050-1200C (1922-2192F) | 1050C (1922F) | 1065-1120C (1949-2048F) | 1082C (1979F) | 1100-1450C (2012-2642F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1100C (2012F) | 1300C (2372F) | 1325C (2417F) | 1330C (2426F) | 1360C (2480F) | | 1420C (2588F) | 1550C (2822F) | 1565C (2849F) | 1650C (3002F) | 1785C (3245F) | 1990C (3614F) | 2300C (4172F) | 2320C (4208F)

1418-1428C (2584-2602F)

Spodumene melts

Related Information

Links

Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy