1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

#1 Q-Rok

Description: 30 mesh silica

Oxide Analysis Formula Tolerance
SiO2 98.00% 1.00
LOI 0.50%n/a
Oxide Weight 60.10
Formula Weight 60.40

Related Information

Links

Materials Silica Sand
Temperatures Quartz inversion (alpha-beta) (540-600)
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.