BORY1 - Bory 1 Crystalline Glaze
CELECG - Celestite Crystalline Glaze
FAAO - Fa's All-Opaque Crystalline Glaze
FAC5 - Crystal Number Five Glaze
FO - Octal Crystalline Glaze
G1214M - 20x5 Cone 6 Base Glossy Glaze
G1214W - Cone 6 Transparent Base
G1214Z1 - Cone 6 Silky CaO matte base glaze
G1215U - Low Expansion Glossy Clear Cone 6
G1216L - Transparent for Cone 6 Porcelains
G1216M - Cone 6 Ultraclear Glaze for Porcelains
G1916Q - Low Fire Highly-Expansion-Adjustable Transparent
G1947U - Cone 10 Glossy transparent glaze
G2000 - LA Matte Cone 6 Matte White
G2240 - Cone 10R Classic Spodumene Matte
G2571A - Cone 10 Silky Dolomite Matte glaze
G2826R - Floating Blue Cone 5-6 Original Glaze Recipe
G2826X - Randy's Red Cone 5
g2851H - Ravenscrag Cone 6 High Calcium Matte Blue
G2853B - Cone 04 Clear Ravenscrag School Glaze
G2896 - Ravenscrag Plum Red Cone 6
G2902B - Cone 6 Crystal Glaze
G2902D - Cone 6 Crystalline Development Project
G2916F - Cone 6 Stoneware/Whiteware transparent glaze
G2926B - Cone 6 Whiteware/Porcelain transparent glaze
G2926J - Low Expansion G2926B
G2928C - Ravenscrag Silky Matte for Cone 6
G2931H - Ulexite High Expansion Zero3 Clear Glaze
G2931K - Low Fire Fritted Zero3 Transparent Glaze
G2931L - Low Expansion Low-Fire Clear
G2934 - Matte Glaze Base for Cone 6
G2934Y - Cone 6 Magnesia Matte Low LOI Version
G3806C - Cone 6 Clear Fluid-Melt transparent glaze
G3838A - Low Expansion Transparent for P300 Porcelain
G3879 - Cone 04 Transparent Low-Expansion transparent glaze
GA10-A - Alberta Slip Base Cone 10R
GA10-B - Alberta Slip Tenmoku Cone 10R
GA10-D - Alberta Slip Black Cone 10R
GA10x-A - Alberta Slip Base for cone 10 oxidation
GA6-A - Alberta Slip Cone 6 transparent honey glaze
GA6-B - Alberta Slip Cone 6 transparent honey glaze
GA6-C - Alberta Slip Floating Blue Cone 6
GA6-D - Alberta Slip Glossy Brown Cone 6
GA6-F - Alberta Slip Cone 6 Oatmeal
GA6-G - Alberta Slip Lithium Brown Cone 6
GA6-G1 - Alberta Slip Lithium Brown Cone 6 Low Expansion
GA6-H - Alberta Slip Cone 6 Black
GBCG - Generic Base Crystalline Glaze
GC106 - GC106 Base Crystalline Glaze
GR10-A - Pure Ravenscrag Slip
GR10-B - Ravenscrag Cone 10R Gloss Base
GR10-C - Ravenscrag Cone 10R Silky Talc Matte
GR10-E - Alberta Slip:Ravenscrag Cone 10R Celadon
GR10-G - Ravenscrag Cone 10 Oxidation Variegated White
GR10-J - Ravenscrag Cone 10R Dolomite Matte
GR10-J1 - Ravenscrag Cone 10R Bamboo Matte
GR10-K1 - Ravenscrag Cone 10R Tenmoku
GR10-L - Ravenscrag Iron Crystal
GR6-A - Ravenscrag Cone 6 Clear Glossy Base
GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue
GR6-C - Ravenscrag Cone 6 White Glossy
GR6-D - Ravenscrag Cone 6 Glossy Black
GR6-E - Ravenscrag Cone 6 Raspberry Glossy
GR6-H - Ravenscrag Cone 6 Oatmeal Matte
GR6-L - Ravenscrag Cone 6 Transparent Burgundy
GR6-M - Ravenscrag Cone 6 Floating Blue
GR6-N - Ravenscrag Alberta Brilliant Cone 6 Celadon
GRNTCG - GRANITE Crystalline Glaze
L2000 - 25 Porcelain
L3341B - Alberta Slip Iron Crystal Cone 10R
L3685U - Cone 03 White Engobe Recipe
L3724F - Cone 03 Terra Cotta Stoneware
L3924C - Zero3 Porcelain Experimental
L3954B - Cone 6 Engobe for Stonewares
L3954N - Cone 10R Base White Engobe Recipe for stonewares
MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
MGBase6 - Zinc Semimatte Glossy Base Cone 6
MGBase7 - Raspberry Cone 6 (Mastering Glazes)
MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
TNF2CG - Tin Foil II Crystalline Glaze
VESUCG - Vesuvius Crystalline Glaze

FO - Octal Crystalline Glaze

Modified: 2022-10-13 21:48:15

Cone 6-9 - Fast-growing crystals variant with dolomite and spodumene

Material Amount
Ferro Frit 311051.00
Zinc Oxide24.00
Silica15.40
Spodumene1.90
Titanium Dioxide2.90
Dolomite4.80
100.00

Notes

From Crystal Glazes Book 1 by Fara Shimbo, page 143.

A general-purpose crystalline glaze meant to grow crystals quickly and mature at a lower temperature than most. This glaze will mature as low as cone 6 and works well with all colorants.

Maturing Cone: 6-9, 10 if you really want it but may not produce as many crystals as at cone 9. At its best at cone 8. Fired to cone 5, it does not form crystals unless seeded.
Crystal number: Moderate.
Rate Of Growth: 1 cm diameter per hour, slightly more on tiles.
Crystal Color: Very White, translucent to opaque. Sometimes bluish.
Crystal Shape: Will flare out when held at a low temperature during a soak. Often has
"pointed" centers, as if one is looking at a volcano from above.
Ground Color: Colorless transparent to ever so vaguely translucent on both tiles and vessels.
Crazing: Varies with crystal growth (more crystals, more crazing), but not too much unless applied very thick. Then crazes like fury.
Color Response: Works well with all colors. Copper in reduction so far has always given red or copper crystals on a turquoise ground.
Seeding properties: Fair with zincite but often grows so many crystals that your pattern may be lost on a tile.

Octal is a very forgiving glaze and produces great crystals over a wide range of maturing temperatures so long as the kiln’s rise to final temperature is fast. I find it better for most uses than Vesuvius (which follows), unless I want the particular crystals that Vesuvius produces.

Related Information

Octal crystal glaze with three colorants


This picture has its own page with more detail, click here to see it.

A vase made from Zen porcelain, about 28 cm tall. Top glazed with Octal + 3% red iron oxide; middle with Octal + 5% manganese dioxide; bottom with Octal + 3% cobalt carbonate. Fired to cone 7, reduced for about three hours.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

XML to Paste Into Insight-live

<?xml version="1.0"?>
<recipes version="1.0" encoding="UTF-8">
<recipe name="Octal Crystalline Glaze" keywords="Cone 6-9 - Fast-growing crystals variant with dolomite and spodumene" id="67" date="2022-10-13" codenum="FO" location="Book 1, Page 143">
<recipelines>
<recipeline material="Ferro Frit 3110" amount="51.000"/>
<recipeline material="Zinc Oxide" amount="24.000"/>
<recipeline material="Silica" amount="15.400"/>
<recipeline material="Spodumene" amount="1.900"/>
<recipeline material="Titanium Dioxide" amount="2.900"/>
<recipeline material="Dolomite" amount="4.800"/>
<url url="https://backup.digitalfire.com/recipe/67" descrip="https://backup.digitalfire.com/recipe/67"/>
</recipelines>
<urls/>
</recipe>
</recipes>