Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

P2O5 (Phosphorus Pentoxide)

Data

Frit Softening Point Sublimates at 300C (From The Oxide Handbook)

Notes

-Phosphorus along with calcium is an essential element in plant and animal growth, thus its principal source is organic ash (i.e. calcined cattle bones).

-Phosphoric oxide is normally present in only trace amounts in ceramic materials.

-It can act as a melter in middle to high fire, but its power-per-unit-added drops drastically beyond 5% additions.

-Small amounts can produce colloidal opacity as in Chinese chun glazes. The depth of Sung glazes is attributed to phosphorus.

-P2O5 is a glass network former like boric oxide and silicon dioxide. Phosphoric glass tends to show as a bluish flush in glazes. It does not enter the silica chain in the matrix. However, P2O5 by itself (with no SiO2 present in the matrix) is a glass former and the base of an entire class of glasses that can be doped with rare earths and metals for produce special purposes ranging from soluble medical implants to insoluble acid-resistance and even radiation resistance.

-Phosphorus can vitrify porcelains without softening and is the key to translucency in bone china.

-Phosphate ions are added to glaze frits as a color control agent during the melting of titania opacified frits.

- P2O5 itself can crystallize in multiple forms. It is known to influence the rate of nucleation and/or crystallization in Li2O and MgO low expansion glaze systems.

-P2O5 combines with certain oxides of iron forms colorless compounds. This suggests that P2O5 could be used to allow the use of less pure materials in glazes and glass.

-Phosphorite mineral Ca3(PO4)2 and Apatite 3Ca3(PO4)2 Ca(Cl,F)2 are the parent rocks of phosphate fertilizers. The latter can thus be used to introduce phosphorus into glazes and frits.

Links

Materials Bone Ash
Materials Phosphorus pentoxide
Materials Hommel Frit 435
Materials Apatite
Materials Borax Decahydrate
Materials Tetrasodium Pyrophosphate Hydrated
Materials Trisodium Phosphate
Materials Sodium Tripolyphosphate
Materials Tricalcium Phosphate
URLs http://en.wikipedia.org/wiki/Phosphate_glass
Phosphate glasses at Wikipedia

Mechanisms

Glaze VariegationPhosphorus can produce variegated and mottling effects in glazes (especially low fire) when used in small amounts (e.g. up to 2%). Bone ash is a source.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy