Description: Calcium Phosphate
Formula: Ca5(PO4)3(OH, F, Cl)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 55.60% | 0.77 | |
| P2O5 | 42.20% | 0.23 | |
| LOI | 2.20% | n/a | |
| Oxide Weight | 75.90 | ||
| Formula Weight | 77.61 | ||
Popular bone-ash substitute. Melts only superficially, has strong opacifying attributes.
Hydroxyapatite Is a refractory and can be used for making crucibles that can survive retreated heat cycles.

This picture has its own page with more detail, click here to see it.
Calcite W Apatite

This picture has its own page with more detail, click here to see it.

This picture has its own page with more detail, click here to see it.
Apatite In Calcite

This picture has its own page with more detail, click here to see it.

This picture has its own page with more detail, click here to see it.
Fluorapatite On Apatite
| URLs |
http://en.wikipedia.org/wiki/Apatite
Apatite at Wikipedia |
| Oxides | P2O5 - Phosphorus Pentoxide |
| Typecodes |
Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials. |
| Hardness (Moh) | 5.0 |
|---|---|
| Frit Softening Point | 1300C D |
| Density (Specific Gravity) | 2.9-3.2 |