Hommel Frit 435

Oxide Analysis Formula Tolerance
Na2O 21.70% 0.47
CaO 1.09% 0.03
Li2O 2.70% 0.12
P2O5 40.14% 0.38
Al2O3 18.85% 0.25
B2O3 6.86% 0.13
SiO2 5.14% 0.12
F 3.52% 0.25
Oxide Weight 134.61
Formula Weight 134.61

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Oxides P2O5 - Phosphorus Pentoxide

Data

Co-efficient of Linear Expansion 15.2 x 10-6
Frit Melting Range (C) 1100F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy