Pyrophyl

Description: Pyrophyllite

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.01
TiO2 0.40% 0.02
Al2O3 22.30% 1.00
SiO2 73.30% 5.58
Fe2O3 0.70% 0.02
LOI 2.80%n/a
Oxide Weight 444.13
Formula Weight 456.93

Notes

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications.

Pyrophyl is a high melting material and is used to reduce hot load deformation and improve volume stability in refractories. It is used in foundry mold and core wash formulations, technical ceramics, structural clay coatings, art pottery.

This material is dry milled and magnetically separated.

The analysis shown here is an average.

Related Information

Links

Materials Alkatrol
Materials Pyrax Pyrophyllite
Materials Pyrophyl R-2253
Materials Pyrophyl R-2252
Materials Pyrophyl R-1404
Materials Pyrophyl R-1403
Materials Sericite Y/T
A commercial grade of sericite mineral.
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Pyrotrol
Materials Pyrofrac
Materials Andafrac
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density lbs/cu. ft. (Packed) 55-70
Pyrometric Cone Equivalent 26-29
Sieve Analysis Dry +200 mesh: 1-12%
Density (Specific Gravity) 2.7-2.75

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy