Andafrac

Description: Andalusite/pyrophyllite

Oxide Analysis Formula Tolerance
Na2O 0.40% 0.02
TiO2 0.40% 0.02
Al2O3 32.00% 1.00
SiO2 63.50% 3.37
Fe2O3 0.70% 0.01
LOI 3.00%n/a
Oxide Weight 309.19
Formula Weight 318.75

Notes

The Andafrac group of mineral products consists of high highly beneficiated Andalusite/Pyrophyllite ores of the best grade available. These products range from coarse grain down to pulverized powders. Volume stability, low hot load deformation and low thermal expansion are characteristic of the high beneficiated ores. The many applications for these products include plastics, castables, kiln car refractories and furnace slag parting compounds.

Three versions are available and they have the same chemistry.
4201 is the coarsest with 53% on 8 mesh.
2001 is dry milled and magnetically separated and is the finest with 4% on 200 mesh. It has a much lower bulk density.
0071 has 65% on 20 mesh.

Related Information

Links

Materials Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings.
Materials Sericite Y/T
A commercial grade of sericite mineral.
Materials Pyrophyl
Materials Pyrofrac
Materials Pyrotrol
Materials Alkatrol
Minerals Andalusite
A low expansion alumina silicate mineral.
Minerals Pyrophyllite
Pyrophyllite is an aluminum silicate mineral with a similar chemical structure to talc (a magnesium
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density lbs/cu. ft. (Packed) 83-112
Frit Softening Point 31 PCE
Density (Specific Gravity) 2.87
Dry M.O.R. (50% Silica) 789C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy