1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Andalusite

Alternate Names: Chiastolite

Oxide Analysis Formula Tolerance
Al2O3 62.90% 1.00
SiO2 37.10% 1.00
Oxide Weight 162.16
Formula Weight 162.16

Notes

As a member of the alumino-silicate Al₂SiO₅ minerals (the polymorphs are kyanite, andalusite, sillimanite). Andalusite has a less densely packed crystal structure than kyanite. It usually begins converting to mullite a little higher than kyanite and does so more gradually. It is thus more volume-stable and (achieving a slight permanent expansion of about 3-5% at around 2730F). Andalusite is often preferred in refractory production because it creates less firing stress, conversion is more controlled and dimensional stability is easier to predict

The andalusite deposit in Hillsboro, NC is very clean with low iron and alkali impurities.

The Pyrofrac series of andalusite phyrophyllite materials are beneficeated to maximize the available andalusite.

Related Information


This picture has its own page with more detail, click here to see it.

Andalusite Cross In Rock

Links

URLs http://en.wikipedia.org/wiki/Andalusite
Andalusite at Wikipedia
Materials Kyanite
A refractory aluminum silicate mineral notable for low thermal expansion and one-way volume expansion as it converts to mullite at high temperatures.
Materials Alkatrol
Materials Pyrofrac
Materials Sericite Y/T
A commercial grade of sericite mineral.
Materials Pyrofrac 4205
Materials Pyrofrac 4203
Materials Pyrofrac 2034
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Andafrac
Materials Pyrofrac 0204
Materials Pyrofrac 0304
Materials Pyrofrac 1004
Materials Pyrofrac 1655
Materials Pyrofrac 1855
Materials Pyrofrac 2023
Materials Pyrofrac 2024
Materials Sillimanite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings.
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.
Typecodes Low Expansion Material
Materials used to make bodies requiring low expansion (e.g. flameware, refractories). The individual particles of these materials have low expansion. Some of theme even expand at certain temperature ranges.
Minerals Andalusite
A low expansion alumina silicate mineral.

Mechanisms

Body Thermal ExpansionVolume stable at high temperatures.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy