| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 4.00% | 0.27 | |
| Na2O | 0.40% | 0.04 | |
| TiO2 | 0.40% | 0.03 | |
| Al2O3 | 16.00% | 1.00 | |
| SiO2 | 72.50% | 7.69 | |
| Fe2O3 | 4.00% | 0.16 | |
| LOI | 2.80% | n/a | |
| Oxide Weight | 620.29 | ||
| Formula Weight | 638.16 | ||
Sericite is the generic mineral name, referring to a very fine-grained white mica, usually composed primarily of muscovite (sometimes with illite or paragonite mixed in).
This is a commercial grade of sericite that has been selected from high-purity deposits, finely ground and classified, and processed to control particle size, brightness, and chemistry.
| Materials |
Pyrotrol
|
| Materials |
Alkatrol
|
| Materials |
Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc. |
| Materials |
Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings. |
| Materials |
Pyrophyl
|
| Materials |
Andafrac
|
| Materials |
Pyrofrac
|
| Minerals |
Sericite
A talc-like mineral (Na2O-K2O).3Al2O3.6SiO2.2H2O. It has a relatively flat, platey grain structure. |
| URLs |
https://www.rescoproducts.com/refractory-products/listing/detail/sericite-y-t
Sericite Y/T product page as RescoProducts.com |
| Pyrometric Cone Equivalent | 14 |
|---|---|
| Density (Specific Gravity) | 2.6 |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |