Pyrotrol

Description: Andalusite/Pyrophyllite Ore

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.02
TiO2 0.40% 0.03
Al2O3 18.90% 1.00
SiO2 77.00% 6.91
Fe2O3 0.40% 0.01
LOI 2.80%n/a
Oxide Weight 524.03
Formula Weight 539.13

Notes

The Pyrotrol group of mineral products offers a controlled blend of milled Andalusite/Pyrophyllite ores designed for use in whiteware ceramic applications. Pyrotrol reduces thermal expansion, stabilizes shrinkage, widens firing range and reduces warpage.

Alumina content is controlled to meet certain specifications. Pyrotrol produces an excellent kiln car wash and is an inexpensive coating material for facebrick production.

This material is dry-milled and magnetically separated.

The practical differences in grade are mainly particle size, bulk density and small chemistry variations:

2253: Standard fine grade: about 1% retained on 200 mesh, 45 pcf bulk density. Chemistry is about 20.5% Al2O3, 75.5% SiO2, 0.4% Fe2O3, 0.4% TiO2.

2254: Similar size and bulk density to 2253, but a slightly different impurity profile: 20.0% Al2O3, 75.0% SiO2, higher Fe2O3 at 0.6%, 0.0% TiO2, and “Other” at 4.0% instead of 2.8%.

3503: Chemically essentially the same as 2253, but finer: 100% -200 mesh and noted as 99% -325 mesh. Its bulk density is lower, 40 pcf instead of 45.

All three show PCE 26, so their refractoriness is listed as the same.

For ceramic use, 2253 and 2254 are similar, while 3503 is the finer version. If substituting in a whiteware body to reduce thermal expansion, improve thermal shock/dunting resistance, stabilize shrinkage or widen firing range, the fired effect should be similar, but the finer 3503 may disperse and react more uniformly and could slightly affect plasticity, water demand, drying shrinkage or slip rheology.

Related Information

Links

Materials Alkatrol
Materials Pyrotrol 2254
Materials Pyrotrol 3503
Materials Pyrotrol 2253
Materials Sericite Y/T
A commercial grade of sericite mineral.
Materials Pyrophyl
Materials Pyrofrac
Materials Andafrac
URLs https://www.rescoproducts.com/docs/default-source/data-sheets-us/sds/pyrotrol-all-grades-msds.pdf?sfvrsn=905bb13b_5
SDS for all versions of Pyrotrol
URLs https://www.rescoproducts.com/docs/default-source/data-sheets-us/pds/pyrotrol-2253-and-2254-and-3503.pdf
Pyrotrol Data Sheet
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density lbs/cu. ft. (Packed) 40-45
Pyrometric Cone Equivalent 26
Sieve Analysis Dry +200 mesh: 1-3.5% +325: 1-12.5%
Density (Specific Gravity) 2.80

Mechanisms

Body Thermal ExpansionPyrotrol products impart higher strength in electrical porcelains and reduce dunting problems associated with traditional porcelain bodies if substituted for silica content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy