Formula: Al2O3.SiO2
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Kyanite
A refractory aluminum silicate mineral notable for low thermal expansion and one-way volume expansion as it converts to mullite at high temperatures. |
| Materials |
Mullite
A highly refractory low-expansion alumino-silicate crystal formed naturally only rarely but produced industrially and within fired kaolin bodies. |
| Materials |
Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings. |
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |
| Minerals |
Sillimanite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings. |
| URLs |
http://en.wikipedia.org/wiki/Sillimanite
Sillimanite at Wikipedia |
| URLs |
http://www.handbookofmineralogy.org/pdfs/Sillimanite.pdf
Sillimanite mineralogy |