Pyrophyl R-2252

Description: Pyrophyllite

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.01
TiO2 0.40% 0.02
Al2O3 26.00% 1.00
SiO2 69.70% 4.55
Fe2O3 0.70% 0.02
LOI 2.80%n/a
Oxide Weight 381.32
Formula Weight 392.31

Notes

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications. The products have shown to be excellent refractory components in foundry mold and core wash formulations. They also perform in electrical porcelain, technical ceramics and structural clay coatings.

Related Information

Links

Materials Pyrophyl R-2253
Materials Pyrophyl R-1403
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Pyrophyl

Data

Bulk Density lbs/cu. ft. (Packed) 70
Pyrometric Cone Equivalent 29
Sieve Analysis Dry +200 mesh: 1%
Density (Specific Gravity) 2.75

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy