Click the link below to go to this page
Video![]() |
Converting G1214M Cone 6 transparent glaze to G1214Z matte
I converted a glossy transparent pottery glaze into a matte glaze using glaze chemistry and recipe logic. Watch me do it in my account at Insight-live.com. We'll cut the Si:Al ratio, increase the CaO further, maintain the thermal expansion for glaze fit and make the recipe shrinkage adjustable using a mix of calcined and raw kaolin. See the landing page to learn every detail: https://digitalfire.com/picture/3787. |