BORY1 - Bory 1 Crystalline Glaze
CELECG - Celestite Crystalline Glaze
FAAO - Fa's All-Opaque Crystalline Glaze
FAC5 - Crystal Number Five Glaze
FO - Octal Crystalline Glaze
G1214M - 20x5 Cone 6 Base Glossy Glaze
G1214W - Cone 6 Transparent Base
G1214Z1 - Cone 6 Silky CaO matte base glaze
G1215U - Low Expansion Glossy Clear Cone 6
G1216L - Transparent for Cone 6 Porcelains
G1216M - Cone 6 Ultraclear Glaze for Porcelains
G1916Q - Low Fire Highly-Expansion-Adjustable Transparent
G1947U - Cone 10 Glossy transparent glaze
G2000 - LA Matte Cone 6 Matte White
G2240 - Cone 10R Classic Spodumene Matte
G2571A - Cone 10 Silky Dolomite Matte glaze
G2826R - Floating Blue Cone 5-6 Original Glaze Recipe
G2826X - Randy's Red Cone 5
g2851H - Ravenscrag Cone 6 High Calcium Matte Blue
G2853B - Cone 04 Clear Ravenscrag School Glaze
G2896 - Ravenscrag Plum Red Cone 6
G2902B - Cone 6 Crystal Glaze
G2902D - Cone 6 Crystalline Development Project
G2916F - Cone 6 Stoneware/Whiteware transparent glaze
G2926B - Cone 6 Whiteware/Porcelain transparent glaze
G2926J - Low Expansion G2926B
G2928C - Ravenscrag Silky Matte for Cone 6
G2931H - Ulexite High Expansion Zero3 Clear Glaze
G2931K - Low Fire Fritted Zero3 Transparent Glaze
G2931L - Low Expansion Low-Fire Clear
G2934 - Matte Glaze Base for Cone 6
G2934Y - Cone 6 Magnesia Matte Low LOI Version
G3806C - Cone 6 Clear Fluid-Melt transparent glaze
G3838A - Low Expansion Transparent for P300 Porcelain
G3879 - Cone 04 Transparent Low-Expansion transparent glaze
GA10-A - Alberta Slip Base Cone 10R
GA10-B - Alberta Slip Tenmoku Cone 10R
GA10-D - Alberta Slip Black Cone 10R
GA10x-A - Alberta Slip Base for cone 10 oxidation
GA6-A - Alberta Slip Cone 6 transparent honey glaze
GA6-B - Alberta Slip Cone 6 transparent honey glaze
GA6-C - Alberta Slip Floating Blue Cone 6
GA6-D - Alberta Slip Glossy Brown Cone 6
GA6-F - Alberta Slip Cone 6 Oatmeal
GA6-G - Alberta Slip Lithium Brown Cone 6
GA6-G1 - Alberta Slip Lithium Brown Cone 6 Low Expansion
GA6-H - Alberta Slip Cone 6 Black
GBCG - Generic Base Crystalline Glaze
GC106 - GC106 Base Crystalline Glaze
GR10-A - Pure Ravenscrag Slip
GR10-B - Ravenscrag Cone 10R Gloss Base
GR10-C - Ravenscrag Cone 10R Silky Talc Matte
GR10-E - Alberta Slip:Ravenscrag Cone 10R Celadon
GR10-G - Ravenscrag Cone 10 Oxidation Variegated White
GR10-J - Ravenscrag Cone 10R Dolomite Matte
GR10-J1 - Ravenscrag Cone 10R Bamboo Matte
GR10-K1 - Ravenscrag Cone 10R Tenmoku
GR10-L - Ravenscrag Iron Crystal
GR6-A - Ravenscrag Cone 6 Clear Glossy Base
GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue
GR6-C - Ravenscrag Cone 6 White Glossy
GR6-D - Ravenscrag Cone 6 Glossy Black
GR6-E - Ravenscrag Cone 6 Raspberry Glossy
GR6-H - Ravenscrag Cone 6 Oatmeal Matte
GR6-L - Ravenscrag Cone 6 Transparent Burgundy
GR6-M - Ravenscrag Cone 6 Floating Blue
GR6-N - Ravenscrag Alberta Brilliant Cone 6 Celadon
GRNTCG - GRANITE Crystalline Glaze
L2000 - 25 Porcelain
L3341B - Alberta Slip Iron Crystal Cone 10R
L3685U - Cone 03 White Engobe Recipe
L3724F - Cone 03 Terra Cotta Stoneware
L3924C - Zero3 Porcelain Experimental
L3954B - Cone 6 Engobe for Stonewares
L3954N - Cone 10R Base White Engobe Recipe for stonewares
MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
MGBase6 - Zinc Semimatte Glossy Base Cone 6
MGBase7 - Raspberry Cone 6 (Mastering Glazes)
MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
TNF2CG - Tin Foil II Crystalline Glaze
VESUCG - Vesuvius Crystalline Glaze

MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)

Modified: 2026-01-04 05:33:48

From page 86 of Mastering Glazes book

Material Amount
Ferro Frit 319520.00
Wollastonite29.00
Nepheline Syenite4.00
EPK30.00
Silica17.00
100.00

Notes

While "Waterfall Brown" is about movement and "Waxwing Brown" is about a waxy feel, HCSM 1 is all about the classic, soft, "eggshell" finish.

Key Properties
• Visual Appearance: A smooth, buttery, semi-matte surface.
• The Science: The matteness comes from Calcium-Silicate crystals that grow as the glaze cools. A controlled cooling cycle ("down-firing") is needed to give the crystals time to form.
• Surface: It is often described as having an "oily" or "buttery" feel rather than a chalky one.
Durability: Resists leaching and staining—making it safer for food surfaces.

Likes (Pros)
• The "Feel": It is pleasant to hold,.
• Reliable Color Canvas: It accepts colorants like Cobalt (blue), Chrome (green), or Manganese (purple) with clarity and soft, variegated transitions.
• No Running: It is a "stiff" melt, staying put and enabling clean lines between different glaze colors.
• Resistant to Staining: The tight crystalline structure of HCSM 1 makes it easy to clean.

Dislikes (Cons)
• Cooling Sensitivity: If your kiln "crash cools", this can come out looking glossy rather than matte. You must be willing to program your kiln to slow down between 1900^circ F and 1500^circ F.
Cutlery Marking: Because the surface is composed of tiny crystals, it can sometimes act like very fine sandpaper against metal.
• Application Thickness: If applied too thick, it can occasionally "crackle" or crawl in corners. If too thin, it loses its buttery feel and can look a bit "stony" or dry.
• Variegated Slate Blue Variation: It is notoriously picky about the specific batch of Red Iron Oxide and Rutile used; shifting from a beautiful blue-grey to a muddy brown.

Related Information

Links

Firing Schedules Mastering Glazes Cone 6
Six-step with controlled drops to 1000C and 760C
Typecodes Recipes from Mastering Glazes Book
Descriptions of these glazes often contain marketing terms over-the-top adjectives like “scientifically formulated”, “perfect”, “exceptional”, “beautifully”, “engineered”, “specifically designed”, “sophisticated”, “flying colors”, etc. Of course there are no perfect recipes to be discovered, they all inhabit spaces balancing a dozen different properties, tuning one most often affects one or more of the others. And, recipe is only one thing affecting the finished product, process factors can have even more influence on finished appearance and properties.
Typecodes Medium Temperature Glaze Recipes
Normally fired at cone 5-7 in electric kilns.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

XML to Paste Into Insight-live

<?xml version="1.0"?>
<recipes version="1.0" encoding="UTF-8">
<recipe name="High Calcium Semimatte 1 (Mastering Glazes)" keywords="From page 86 of Mastering Glazes book" id="41" date="2026-01-04" codenum="MGBase1">
<recipelines>
<recipeline material="Ferro Frit 3195" amount="20.000"/>
<recipeline material="Wollastonite" amount="29.000"/>
<recipeline material="Nepheline Syenite" amount="4.000"/>
<recipeline material="EPK" amount="30.000"/>
<recipeline material="Silica" amount="17.000"/>
<url url="https://backup.digitalfire.com/recipe/41" descrip="https://backup.digitalfire.com/recipe/41"/>
</recipelines>
<urls/>
</recipe>
</recipes>
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved