Ultrox

Description: Zirconium Silicate Glaze Opacifier

Oxide Analysis Formula Tolerance
ZrO2 65.00% 1.00
SiO2 35.00% 1.10
Oxide Weight 189.57
Formula Weight 189.57

Notes

Ultrox is a brand name for zircon. Multiple grades are available.

Ultrox opacifiers intended for glazes are claimed to assure uniformity of opacity, texture and color over a wide range of temperatures and compositions. They reduce the expansion of glazes and tend to reduce crazing. They increase the resistance of glazes to chemical attack and widen the firing range. Ultrox melts at 4000F and has a coefficient of thermal expansion of 42 x 10-7, a hardness of 7.5 Moh and index of refraction of 2. It is composed of 65% ZrO2 and 35% SiO2 in a formula of ZrO2:SiO2.

Ultrox is used for the production of both white and color glazes for sanitary ware, wall tile, glazed brick, structural tile, stoneware, dinnerware and special porcelains. It is used in amount of 12-20% of the glaze batch.

-Ultrox has an average particle size of 2 microns.
-Ultrox 500W has an average particle size of 1 micron and thus provides greater whitening power. It lightens color appreciably and thus requires more stain.
-Ultrox 1000W has an average particle size of .5 micron and provides the maximum reflectance and opacity.

Ultrox has an extremely high melting point and low uniform thermal expansion and can thus be slip cast or pressed to produce zirconium silicate refractories (for use in glass melting furnaces, foundries, refractory porcelains, washes for refractory slabs, refractory cements). Compositions of Ultrox alone can approach the theoretical density of zircon.

Coefficient of thermal expansion: 42 x 10 -7
Hardness: 7.5 Moh's scale
Index of refraction: 2

Ultrox products are relatively non-hazardous based on plant operating experience. Avoid inhalation of dust. May cause eye irritation on repeated contact.

Ultrox is zirconium silicate, thus the same as Zircopax Plus or Superpax. Although a finer particle size.

Related Information

Ultrox 500W original container bags


This picture has its own page with more detail, click here to see it.

Ultrox Original Container Bag


This picture has its own page with more detail, click here to see it.

These bags actually contain Zircopax Plus since Trebol is the new owner of the company.

Links

URLs http://www.atofinachemicals.com/plants/canada/pdf/ds/773.PDF
MSDS
URLs https://www.gtrebol.com/PDF/T-FLORIDA-ULTROX-Z-ES-HS.pdf
Ultrox Z+ dry-milled Zircon for sanitaryware glazes
URLs https://www.gtrebol.com/PDF/T-FLORIDA-ULTROXS.pdf
Ultrox S dry-milled Zircon for sanitaryware glazes
URLs https://www.gtrebol.com/PDF/T-FLORIDA-ULTROX-325-ES-HS.pdf
Ultrox 325 mesh data sheet
URLs https://www.gtrebol.com/PDF/Ultrox%20(all%20grades)GHS%20REV%2010.pdf
Ultrox SDS Safety Data Sheet
Materials Zircopax Plus
Materials Superpax
Materials Opax
Materials Zircon
Typecodes Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms).

Data

Frit Softening Point 2200C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy