Description: Zirconium Oxide, Zirconia

Oxide Analysis Formula Tolerance
Na2O 1.11% 1.00
ZrO2 90.84% 41.18
Al2O3 0.91% 0.50
SiO2 6.48% 6.02
Oxide Weight 5,548.72
Formula Weight 5,548.72

Notes

Opax is a brand-name product, it is actually zirconia (zirconium dioxide), Zircopax is a brand-name of zircon (zirconium silicate). Both are used as opacifiers. Zircon is the natural source material from which zirconia is made. Opax does not opacify any better than zircopax, but it is more expensive. And it mattes glazes much more.

Related Information

Links

Materials Ultrox
Materials Zircon
Zircon (zirconium silicate) is a hard, dense, refractory ceramic material used to opacify pottery glazes and in refractory products such as kiln washes, crucibl
Materials Zircopax Plus
Typecodes Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy