Pemco Frit P-25

Alternate Names: Pemco 25, Pemco Frit 25

Description: Leadless alkaline fluorine frit, use for cone 06-02

Oxide Analysis Formula Tolerance
CaO 0.50% 0.03
K2O 5.40% 0.18
Na2O 14.70% 0.76
ZnO 0.70% 0.03
B2O3 16.90% 0.78
Al2O3 12.10% 0.38
SiO2 49.70% 2.65
F 1.80% 0.30
Oxide Weight 326.35
Formula Weight 326.35

Notes

Often used with 10% clay addition for low temperature crackle glazes. Frequently used as a component in partially fritted wall tile glazes.

Related Information

Links

Materials Hommel Frit 25
Materials Fusion Frit F-225
Materials Ferro Frit 3269
Materials General Frit GF-114
Materials Hommel Frit 259
Materials Ferro Frit 3819
Materials Fusion Frit FZ-25
Materials Pemco Frit Pb-106
Materials Pemco Frit P-2D71
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.0 x 10-6 (50-450C)
Frit Melting Range (C) 1320-1420F
I.F.P. (celsius) 575C