Fusion Frit FZ-25

Alternate Names: Frit FZ25

Description: Boro Sodium Frit, Tile Flux

Oxide Analysis Formula Tolerance
CaO 0.50% 0.03
K2O 5.40% 0.18
Na2O 14.70% 0.76
ZnO 0.70% 0.03
B2O3 16.90% 0.78
Al2O3 12.10% 0.38
SiO2 49.70% 2.65
Oxide Weight 320.58
Formula Weight 320.58

Related Information

Links

Materials Ferro Frit 3269
Materials Hommel Frit 259
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3819
Materials Pemco Frit P-25
Materials General Frit GF-114
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.84
Frit Softening Point 790C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy