| Monthly Tech-Tip | No tracking! No ads! | |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 1.00% | 1.00 | |
| ZrO2 | 1.00% | 0.49 | |
| Fe2O3 | 1.00% | 0.38 | |
| TiO2 | 97.00% | 72.96 | |
| Oxide Weight | 6,010.00 | ||
| Formula Weight | 6,010.00 | ||
Processed rutile ore (upgraded to 95%+ TiO2 by smelting). Available in a variety of sizes. It can be used at a speckling agent in glazes, however it settles quickly because of the high specific gravity. It can also be used as a speckling agent in bodies, try around 0.2% to start.

This picture has its own page with more detail, click here to see it.
Yes, the granular and powdered grades of pure rutile are the same material. But, for producers, the milling process it is very difficult because the raw mineral is so hard. Commercial ceramic grade powder is minus 325 mesh, the companies doing this obviously have very good grinding equipment. They also have patience because even in this efficient porcelain ball mill, 90 minutes was only enough to get 50% to minus 325 mesh! The color of the powder is a good indication of its quality, the finer the grind the lighter tan it will be. That means you can use the color to gauge the mesh size. And, if you have a ball mill you can milled it more if needed.

This picture has its own page with more detail, click here to see it.
Clearly, the manganese is blossoming and producing far better speckle than the other two.
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Materials |
Rutile
A raw TiO2-containing mineral used in ceramics to color and variegate glaze surfaces. |
| Materials |
Ilmenite
|
| Materials |
Granular Ilmenite
|
| Materials |
Manganese Granular
In ceramics, it is used primarily in clays and glazes to achieve fired speckle (including the brick industry). |
| Materials |
Magnetite Granular
|
| Materials |
Ceramic Rutile
Rutile mineral ground to a very fine particle size (e.g. 325 mesh) contributes titanium and iron that colors and variegates ceramic glazes. |
| Glaze Variegation | Granular rutile is popular as a specking agent. Start with 0.2%. This material is heavy and will settle in glaze with a thin slurry. |
|---|