Alternate Names: FERROSO-FERRIC OXIDE, FEROSIC OXIDE
Formula: Fe3O4
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 66.17% | 1.00 | |
| FeO | 33.83% | 1.00 | |
| Oxide Weight | 241.80 | ||
| Formula Weight | 241.80 | ||
It is not to be confused with brown Fe3O4 mixed ferrous-ferric iron oxide. Unlike the much softer black and red iron oxide, this material is useful in granular form to introduce specking into bodies and glazes. Many other materials are available as speckling agents.
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Minerals |
Magnetite
A black, hard, dense and stable crystalline mineral form of iron oxide. |
| Minerals |
Iron Pyrite
Iron pyrite, or Fool's Gold, is a common metallic mineral containing about 50% iron and 33% sulfur. |
| Materials |
Manganese Granular
In ceramics, it is used primarily in clays and glazes to achieve fired speckle (including the brick industry). |
| Materials |
Granular Rutile
The same material as milled rutile, but ground only to granular size. |
| Materials |
Granular Ilmenite
|
| Hardness (Moh) | 6.5 |
|---|---|
| Frit Softening Point | 1538C D |
| Density (Specific Gravity) | 5.18 |