Sericite Y/T

Oxide Analysis Formula Tolerance
K2O 4.00% 0.27
Na2O 0.40% 0.04
TiO2 0.40% 0.03
Al2O3 16.00% 1.00
SiO2 72.50% 7.69
Fe2O3 4.00% 0.16
LOI 2.80%n/a
Oxide Weight 620.29
Formula Weight 638.16

Notes

Sericite is the generic mineral name, referring to a very fine-grained white mica, usually composed primarily of muscovite (sometimes with illite or paragonite mixed in).

This is a commercial grade of sericite that has been selected from high-purity deposits, finely ground and classified, and processed to control particle size, brightness, and chemistry.

Related Information

Links

Materials Pyrotrol
Materials Pyrofrac
Materials Andafrac
Materials Pyrophyl
Materials Andalusite
A low expansion aluminum silicate mineral that converts to mullite on repeated firings.
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Alkatrol
Minerals Sericite
A talc-like mineral (Na2O-K2O).3Al2O3.6SiO2.2H2O. It has a relatively flat, platey grain structure.
URLs https://www.rescoproducts.com/refractory-products/listing/detail/sericite-y-t
Sericite Y/T product page as RescoProducts.com

Data

Pyrometric Cone Equivalent 14
Density (Specific Gravity) 2.6

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy