Superpax

Description: Zirconium silicate

Oxide Analysis Formula Tolerance
ZrO2 67.21% 1.00
SiO2 32.79% 1.00
Oxide Weight 183.34
Formula Weight 183.34

Notes

Also known as Zircopax Plus or Ultrox (see link below for more information).