Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

Sb2O3 (Antimony Oxide)

Notes

-Antimony oxide is used as an opacifier in low fire glazes and porcelain enamel (mainly leadless but it has been replaced to an extent by titania). Antimony is easily reducible; thus an oxidizing agent like potassium nitrate may be required to prevent it from going into solution and losing its opacifying power and affecting color.

-It is not useful in glazes over cone 1 due to volatilization.

-Antimony can be used as a yellow body stain in combination with rutile or titanium.

-Antimony will bleach the surface of low fire red-burning clay to a buff color to produce variegated coloration.

-The glass industry uses antimony as a decolorizing and fining agent to clarify glasses and as a stabilizing agent in the production of emerald green glass.

-Antimony has a low thermal expansion and reduces crazing.

Links

Materials Antimony Oxide
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Temperatures Antimony volatilizes (1100-)

Mechanisms

Glaze ColorIt can give a yellowish color if the glaze contains lead, this is a result of the precipitation of yellow lead antimonate (known as Naples yellow).
Glaze OpacifierAntimony works to a limited extent as an opacifier to cone 1.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy